MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips MarFlex® 1125 Polyethylene; LDPE  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Low density polyethylene. This LDPE is tailored for blown film applications that require:
  • Good impact
  • No slip, includes antiblock
  • Good processability
  • Good sealability
  • Good drawdown

Applications: Typical blown film applications include:

  • Liners
  • Trash bags
  • Converter films

Information provided by Phillips

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³ASTM D-1505
Water Vapor Transmission 15.0 g/m²/day0.966 g/100 in²/dayBlown Film at 1.25 mil; ASTM F-1249
Oxygen Transmission Rate 5200 cc/m²/day335 cc/100 in²/dayBlown Film at 1.25 mil; ASTM D-3985
Melt Index of Compound 2.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.1 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Antiblock Level 4000 ppm4000 ppm
Slip Level 0.00 ppm0.00 ppm
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.550.55Blown Film at 1.25 mil; ASTM D-1894
Elmendorf Tear Strength, MD 4.92 g/micron125 g/milBlown Film at 1.25 mil; ASTM D-1922
Elmendorf Tear Strength, TD 3.94 g/micron100 g/milBlown Film at 1.25 mil; ASTM D-1922
Dart Drop 3.15 g/micron80.0 g/milBlown Film at 1.25 mil; ASTM D-1709
 
Thermal PropertiesMetricEnglishComments
Melting Point 107 °C225 °FASTM D-3418
Vicat Softening Point 96.0 °C205 °FASTM D-1525
 
Optical PropertiesMetricEnglishComments
Haze 9.0 %
@Thickness 0.0317 mm
9.0 %
@Thickness 0.00125 in
blown films; ASTM D-1003
Gloss 80 %80 %60°, Blown Film at 1.25 mil; ASTM D-2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carmel Olefins Ipethene® 670 Low Density Polyethylene
Arkema LOTRYL® 7 BA 01 Copolymer Ethylene - Butyl Acrylate
Arkema LOTADER® 3210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Dow 4012 Low Density Polyethylene (LDPE)
Dow VERSIFY™ 2000 Plastomer

PCHEVD222 / 20716

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.