MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® C40 LN 07 0.04 mm Blown Film Cold Air
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA)

Material Notes:

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 - 1.15 g/cc0.0405 - 0.0415 lb/in³
Water Vapor Transmission 25.0 g/m²/day1.61 g/100 in²/day85% RH
Oxygen Transmission Rate 14.0 cc/m²/day0.902 cc/100 in²/day50% RH
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psiTD
 70.0 MPa10200 psiMD
Elongation at Break 475 %475 %MD
 480 %480 %TD
Tensile Modulus 0.600 GPa87.0 ksiTD
 0.600 GPa87.0 ksiMD
 
Thermal PropertiesMetricEnglishComments
Melting Point 189 °C372 °F
 
Descriptive Properties
Commercial StatusEurope
Film Grade1-3BASF
Lubricant250 - 550 mg/kgBASF

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® C40 LN 01 PA6/66
BASF Ultramid® C33 01 PA66/6 (Conditioned)
BASF Ultramid® C33L 01 PA66/6 (Dry)
BASF Ultramid® C33 01 PA66/6 (Dry)
Dura-Bar G2 Continuously Cast Gray Iron Bar Stock ASTM A48

PBASG0350 / 131983

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.