MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

AISI 4023 Steel, normalized at 925°C (1700°F), machined to 25 mm (1 in.) rounds, pseudocarburized at 925°C (1700°F) and oil quenched, 150°C (300°F) temper

Most of the data in MatWeb has been supplied directly by companies in the supply chain - the manufacturers, or, less commonly, distributors or fabricators. Other data has been provided by standards organizations or from similar materials/known relationships by the MatWeb staff. For more information about this specific material, see the following source(s):


ASM Metals Reference Book, Third edition, Michael Bauccio, Ed. ASM International, Materials Park, OH, 1993.

ASM Specialty Handbook - Carbon and Alloy Steels, edited by J.R. Davis, Davis & Associates, ASM International, Metals Park, OH, (1996).

Engineering Properties of Steels, Philip D. Harvey, editor, American Society for Metals, Metals Park, OH, (1982).

Metals Handbook, Vol.1 - Properties and Selection: Irons, Steels, and High-Performance Alloys, ASM International 10th Ed. 1990.

Metals Handbook, Howard E. Boyer and Timothy L. Gall, Eds., American Society for Metals, Materials Park, OH, 1985.

Physics for Scientists and Engineers with Modern Physics, 2nd ed., Douglas C. Giancoli, Prentice Hall Publishers, Englewood Cliffs, NJ (1989)

SAE Ferrous Materials Standards Manual, 1999 ed., HS-30, Society of Automotive Engineers, Inc., Warrendale, PA, (1999).

ASTM Standards in ACI 301, 318, and 349, Publication SP-71, American Society for Testing and Materials, Philadelphia, PA, (1980)

Worldwide Guide to Equivalent Irons and Steels, 4th Ed., ASM Material Data Series, ASM International, Materials Park, OH, (2000)


Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.