AISI Type S21900 (21-6-9) Stainless Steel, 15% final cold reduction, stress relieved 620°C (1150°F) for 2 hours, air cooled
Most of the data in MatWeb has been supplied directly by companies in the supply chain -
the manufacturers, or, less commonly, distributors or fabricators. Other data
has been provided by standards organizations or from similar materials/known relationships by
the MatWeb staff. For more information about this specific material, see the following source(s):
ASM Metals Reference Book, Third edition, Michael Bauccio, Ed. ASM International, Materials Park, OH, 1993.
Engineering Properties of Steels, Philip D. Harvey, editor, American Society for Metals, Metals Park, OH, (1982).
Metals Handbook, Howard E. Boyer and Timothy L. Gall, Eds., American Society for Metals, Materials Park, OH, 1985.