System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Drill Down to All Materials Data Sheets
This series of pages is an inefficient set of links to all data sheets in MatWeb. We have several search tools, listed above, that give you more efficient methods to reach the information that you need.
Replacing...
Total Evatane® 28 - 03 HDPE, blown film
Total Evatane® 28 - 05 HDPE vinyl acetate copolymer, blown film, injection molding
Total FE 8000 LDPE blown film
Total FE 8004 LDPE blown film
Total Finaclear® 520 Clear Impact Polystyrene
Total Finaclear® 521 Clear Impact Polystyrene
Total Finaclear® 530 Clear Impact Polystyrene
Total Finaclear® MBF Clear Impact Polystyrene
Total Finaplas® 1251 Copolymer Syndiotactic Polypropylene
Total Finaplas® 1471 Copolymer Syndiotactic Polypropylene
Total Finaplas® 1571 Copolymer Syndiotactic Polypropylene
Total Finaprene® 1205 Di-block Styrene-Butadiene TPE Copolymer
Total Finaprene® 401 Styrene-Butadiene TPE Copolymer
Total Finaprene® 401 Thermoplastic Elastomer
Total Finaprene® 409 Styrene-Butadiene TPE Copolymer
Total Finaprene® 409 Thermoplastic Elastomer
Total Finaprene® 411 Thermoplastic Elastomer
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 57 Shore A
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 58 Shore A
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 59 Shore A
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 61 Shore A
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer, 80 Shore A
Total Finaprene® 411x Thermoplastic Elastomer
Total Finaprene® 416 Styrene-Butadiene TPE Copolymer
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 54 MFI
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 56 MFI
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 79 MFI
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 84 MFI
Total Finaprene® 436 Thermoplastic Elastomer
Total Finaprene® 502 Styrene-Butadiene TPE Copolymer
Total Finaprene® 503 Styrene-Butadiene TPE Copolymer
Total Finaprene® 507 Styrene-Butadiene TPE Copolymer
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 57 Shore A
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 58 Shore A
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 59 Shore A
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 61 Shore A
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 62 Shore A
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer, Uncompounded
Total Finaprene® 602 Thermoplastic Elastomer
Total Finaprene® 602D Clear Impact Polystyrene
Total Finaprene® SX 2309 Thermoplastic Elastomer
Total Finathene® 1288 HDPE film
Total Finathene® 2344 HDPE film
Total Finathene® 3344N Natural HDPE pipe grade
Total Finathene® 3407B Black HDPE pipe grade
Total Finathene® 3802N Natural HDPE pipe grade
Total Finathene® 4344 HDPE, blow molding
Total Finathene® 50100.3 HDPE blow molding
Total Finathene® 5302 HDPE drain tile, corrugated pipe resin
Total Finathene® 53080 HDPE, blow molding, sheet
Total Finathene® 53140 HDPE, blow molding, sheet
Total Finathene® 56020 HDPE, blow molding, sheet
Total Finathene® 6002 HDPE, blow molding, pipe
Total Finathene® 6006 HDPE, blow molding, pipe
Total Finathene® 6450 HDPE film
Total Finathene® 7208 HDPE extrusion resin
Total Finathene® CD 481 HDPE conduit
Total Finathene® CD 522 HDPE corrugated pipe resin
Total Finathene® DF 210 HDPE resin
Total Finathene® HL 328 HDPE resin
Total Finathene® LL 4010 FE 18 LLDPE film
Total Finathene® LL 4010 FH 18 LLDPE film
Total Finathene® LL 6010 FE 18P LLDPE film
Total Finathene® LL 6010 FH 18P LLDPE film
Total Finathene® RS 528 HDPE blow molding
Total Finathene® SI 508 HDPE blow molding
Total Finathene® SR 572 HDPE blow molding
Total Finathene® WR 201 B HDPE blow molding
Total Finathene® WR 201 B N HDPE blow molding
Total HD 5809 S01 High Density Polyethylene - Monofilament Extrusion
Total HD 6081 High Density Polyethylene - Injection Molding
Total HD 6221 High Density Polyethylene - Blow Molding
Total HL 717 High Density Polyethylene - Blown Film
Total HP 401 MDPE, pipe, cable, sheet
Total HP 401N Natural HDPE, pipe
Total HT 514 MDPE film
Total Impact Polystyrene 940E Super High Impact Polystyrene, Sheet Extrusion and Thermoforming Grade
Total Lacqrene® 1070 Crystal Polystyrene
Total Lacqrene® 1160(AS) Crystal Polystyrene
Total Lacqrene® 1235 High Impact Polystyrene
Total Lacqrene® 1240 Crystal Polystyrene
Total Lacqrene® 1250 Crystal Polystyrene
Total Lacqrene® 2551 Medium Impact Polystyrene
Total Lacqrene® 2901 Medium Impact Polystyrene
Total Lacqrene® 3351(AS) Impact Polystyrene
Total Lacqrene® 3351(EU) Impact Polystyrene
Total Lacqrene® 4240(AS) High Impact Polystyrene
Total Lacqrene® 4240(EU) High Impact Polystyrene
Total Lacqrene® 4241 High Impact Polystyrene
Total Lacqrene® 4431 Flame Retardant Polystyrene
Total Lacqrene® 4801
Total Lacqrene® 6630 Impact Polystyrene
Total Lacqrene® 6631 Impact Polystyrene
Total Lacqrene® 740 High Impact Polystyrene
Total Lacqrene® 814(AS) High Impact Polystyrene
Total Lacqrene® 814(EU) High Impact Polystyrene
Total Lacqrene® 851 High Impact Polystyrene
Total Lacqrene® 852 High Impact Polystyrene
Total Lacqrene® 9218 Polystyrene
Total Lacqtene® 1003 FE 30 HDPE, blow molding
Total Lacqtene® 1008 FE 30 LDPE blown film
Total Lacqtene® 1025 FH 24 LDPE blown film
Total Lacqtene® 2001 PBK 44 HDPE pipe
Total Lacqtene® 2001 TBK 40 HDPE pipe
Total Lacqtene® 2001 TBK 46 HDPE pipe
Total Lacqtene® 2001 TBL 46 HDPE pipe
Total Lacqtene® 2001 TMA 46 HDPE pipe
Total Lacqtene® 2001 TN 46 HDPE pipe
Total Lacqtene® 2001 TYL 46 HDPE pipe
Total Lacqtene® 2002 TBL 40 HDPE pipe
Total Lacqtene® 2002 TN 40 HDPE, blow molding, pipe, sheet
Total Lacqtene® 2002 TYL 40 HDPE pipe
Total Lacqtene® 2003 PBK 41 HDPE pipe, sheet
Total Lacqtene® 2004 TN 52 HDPE pipe
Total Lacqtene® 2005 TN 59 HDPE pipe
Total Lacqtene® 2006 PBK 35 HDPE pipe, sheet
Total Lacqtene® 2006 TN 35 HDPE pipe coating
Total Lacqtene® 2007 TN 61 HDPE pipe
Total Lacqtene® 6002 FLG 42 HDPE film
Total Lacqtene® FB 3010 LDPE blown film
Total Lacqtene® FD 0270 LDPE, blown film, compounding, injection molding
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film
Total LDPE 1070 MN 18 C Low Density Polyethylene - Injection Molding and Compounding
Total LDPE 1200 MN 18 C Low Density Polyethylene - Injection Molding and Compounding
Total LDPE 1700 MN 18 C Low Density Polyethylene - Injection Molding and Compounding
Total LDPE LA 0710 Low Density Polyethylene - Extrusion Coating
Total LDPE LD 0304 Low Density Polyethylene - Extrusion Coating
Total LF 38 YS CF MDPE, pipe
Total LLDPE LL 1810 H Linear Low Density Polyethylene - Blown Film
Total LLDPE LL 1810 Linear Low Density Polyethylene - Blown Film
Total LLDPE LL 1820 H Linear Low Density Polyethylene - Blown Film
Total LLDPE LL 1820 Linear Low Density Polyethylene - Blown Film
Total Lotrene® Q1018H Linear Low Density Polyethylene, Blown Film
Total Lotrene® Q1018N Linear Low Density Polyethylene, Blown Film
Total Lotrene® Q2018C Linear Low Density Polyethylene, Blown Film
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film
Total Lumicene® M6040 Metallocene High Density Polyethylene
Total Lumicene® mPE M 2310 EP Metallocene Polyethylene, Blown Film
Total Lumicene® mPE M 2704 EP S01 Metallocene Polyethylene, Blown Film
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Blown Film
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film
Total Lumicene® mPE M 3410 EP HDPE Film
Total Lumicene® mPE M 3427 Metallocene Polyethylene, Cast Film
Total Lumicene® mPE M 3509 Medium Density Polyethylene, Blow Molding
Total Lumicene® mPE M 4040 Metallocene Polyethylene, Cast Film
Total Lumicene® mPE M 4041 UV Metallocene Polyethylene, Rotomolding
Total Lumicene® mPE M 4707 EP Metallocene Polyethylene, Blown Film
Total Lumicene® mPE M 5220 High Density Polyethylene, Blow Molding
Total Lumicene® mPE M5220 M Metallocene High Density Polyethylene
Total Lumicene® mPE M5220 Metallocene High Density Polyethylene
Total Lumicene® mPE M5510 EP Metallocene Polyethylene, Blown Film
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film
Total Lumicene® MR 2001 Polypropylene, Metallocene Polypropylene
Total Lumicene® MR 2002 Polypropylene, Metallocene Polypropylene
Total Lumicene® MR10MX0 Metallocene Random Copolymer Polypropylene, Injection Molding and Injection Blow Molding
Total Lumicene® MR110MC2 Metallocene Random Copolymer Polypropylene, Injection Molding
Total Lumicene® MR30MC2 Metallocene Random Copolymer Polypropylene, Injection Molding
Total Lumicene® MR30MX0 Metallocene Random Copolymer Polypropylene, Injection Molding and Injection Blow Molding
Total Lumicene® MR60MC2 Metallocene Random Copolymer Polypropylene, Injection Molding
Total MDPE 3802 B Medium Density Polyethylene, Cable
Total MDPE 3802 B Medium Density Polyethylene, Pipes & Fittings
Total MDPE 3802 Blue Medium Density Polyethylene, Stripes
Total MDPE 3802 Medium Density Polyethylene, Blow Molding
Total MDPE 3802 Medium Density Polyethylene, Cable
Total MDPE 3802 YCF Medium Density Polyethylene, Pipes & Fittings
Total MDPE HF 513 Medium Density Polyethylene, Blown Film
Total MDPE HR 515 Medium Density Polyethylene, Blown Film
Total MDPE HT 514 Medium Density Polyethylene, Blown Film
Total MDPE LF 38 YS CF Medium Density Polyethylene, Stripes
Total MS 201 B HDPE blow molding
Total MS 201 B N HDPE blow molding
Total MS201 BN-NA High Density Polyethylene - Fuel Tank Resin
Total Polystyrene Impact 3450 Aesthetic, High Fluidity, High Heat Resistance, High Impact Polystyrene
Total Polystyrene Impact 6540 Easy Flow Impact Polystyrene
Total Polystyrene Impact 8260 Improved Environmental Stress Crack Resistance High Impact Polystyrene
Total PPC 10641 Polypropylene, Heterophasic Copolymer, Injection Molding
Total PPC 10642 Polypropylene, Heterophasic Copolymer, Injection Molding
Total PPC 10710 Polypropylene, Heterophasic Copolymer
Total PPC 10712 Polypropylene, Heterophasic Copolymer
Total PPC 11642 Polypropylene, Heterophasic Copolymer, Injection Molding
Total PPC 11712 Polypropylene, Heterophasic Copolymer
Total PPC 11750 Polypropylene, Heterophasic Copolymer, Injection Molding
Total PPC 11812 S01 Polypropylene, Heterophasic Copolymer, Injection Molding
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding
Total PPC 12712 Polypropylene, Heterophasic Copolymer
Total PPC 13442 Polypropylene, Heterophasic Copolymer
Total PPC 13712 Polypropylene, Heterophasic Copolymer
Total PPC 13812 Polypropylene, Heterophasic Copolymer, Injection Molding
Total PPC 1640 Polypropylene, Heterophasic Copolymer, Non-pressure Pipes
Total PPC 1645 Polypropylene, Heterophasic Copolymer, Pipes
Total PPC 2660 Polypropylene, Heterophasic Copolymer
Total PPC 3020 GN3 Polypropylene, Random Copolymer
Total PPC 3060 MW5 Polypropylene, Heterophasic Copolymer, Automotive
Total PPC 3120 MU5 Polypropylene, Heterophasic Copolymer, Automotive
Total PPC 3150 MX5 Polypropylene, Heterophasic Copolymer, Automotive
Total PPC 3640 Polypropylene, Heterophasic Copolymer
Total PPC 3645 Polypropylene, Heterophasic Copolymer
Total PPC 3650 Polypropylene, Heterophasic Copolymer, Injection Molding
Total PPC 3660 Polypropylene, Heterophasic Copolymer
Total PPC 3666 Polypropylene, Heterophasic Copolymer, Extrusion
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade
Total PPC 4252 Polypropylene, Impact Copolymer Corrugated Sheet
Total PPC 4280W Polypropylene, Impact Copolymer
Total PPC 4481WZ Polypropylene, Impact Copolymer
Total PPC 4524WZ Polypropylene, Impact Copolymer
Total PPC 4624WZ Polypropylene, Impact Copolymer
Total PPC 4640 Polypropylene, Heterophasic Copolymer
Total PPC 4660 Polypropylene, Heterophasic Copolymer
Total PPC 4663 Polypropylene, Heterophasic Copolymer
Total PPC 4720 WZ Polypropylene, Impact Copolymer
Total PPC 4720XWZ Polypropylene, Impact Copolymer
Total PPC 4820WZ Polypropylene, Impact Copolymer
Total PPC 4824WZ Polypropylene, Impact Copolymer
Total PPC 4920WZ Polypropylene, Impact Copolymer
Total PPC 4944CWZ Polypropylene, Impact Copolymer
Total PPC 4944WZ Polypropylene, Impact Copolymer
Total PPC 5571 Polypropylene, Impact Copolymer Injection Molding
Total PPC 5660 Propylene, Heterophasic Copolymer
Total PPC 5720WZ Polypropylene, Impact Copolymer
Total PPC 5724 Polypropylene, Extra High Impact Copolymer
Total PPC 5752 Polypropylene, Heterophasic Copolymer
Total PPC 5945WZ Polypropylene, Impact Copolymer
Total PPC 5946WZ Polypropylene, Impact Copolymer
Total PPC 7612 Polypropylene, Heterophasic Copolymer
Total PPC 7642 Polypropylene, Heterophasic Copolymer
Total PPC 7650 Polypropylene, Heterophasic Copolymer
Total PPC 7652 Polypropylene, Heterophasic Copolymer, Injection Molding
Total PPC 7712 Polypropylene, Heterophasic Copolymer
Total PPC 7760 Polypropylene, Heterophasic Copolymer
Total PPC 7810 Polypropylene, Heterophasic Copolymer, High Impact
Total PPC 8780 Polypropylene, Heterophasic Copolymer, Injection Molding
Total PPC 9610 Polypropylene, Heterophasic Copolymer
Total PPC 9612 Polypropylene, Heterophasic Copolymer, Injection Molding
Total PPC 9642 Polypropylene, Heterophasic Copolymer
Total PPC 9712 Polypropylene, Heterophasic Copolymer
Total PPC 9760 Polypropylene, Heterophasic Copolymer
Total PPC M6823MZ Metallocene Isostatic Propylene Polymer
Total PPH 10012 Polypropylene, Homopolymer
Total PPH 10042 Polypropylene, Homopolymer
Total PPH 10060 Polypropylene, Homopolymer
Total PPH 10069 Polypropylene, Homopolymer
Total PPH 10080 Polypropylene, Homopolymer
Total PPH 10099 Polypropylene, Homopolymer
Total PPH 11012 Polypropylene Homopolymer, Injection Molding
Total PPH 12020 Polypropylene Homopolymer, Injection Molding
Total PPH 3051 Polypropylene, Homopolymer
Total PPH 3060 Polypropylene, Homopolymer
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.