Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Drill Down to All Materials Data Sheets
This series of pages is an inefficient set of links to all data sheets in MatWeb. We have several search tools, listed above, that give you more efficient methods to reach the information that you need.
Replacing...
RTP Company RTP 207 G HS L Nylon 4/6 (PA), Glass Fiber - Heat Stabilized - Lubricated - Dry As Molded
RTP Company RTP 207 H HS MS 2 Nylon 6/6 (PA), Glass Fiber - Impact Modified - Molybdenum Disulfide - Heat Stabilized - Preliminary Data
RTP Company RTP 207 H Impact-Modified Nylon 6/6 (PA), Glass Fiber
RTP Company RTP 207 HB Nylon 6/6 (PA), Glass Fiber - UL94 HB
RTP Company RTP 207 HS Nylon 6/6 (PA 6/6) Glass Fiber 40% - Heat Stable
RTP Company RTP 207 HS MS 2 Nylon 6/6 (PA), Glass Fiber - Heat Stabilized - Molybdenum Disulfide
RTP Company RTP 207 HS Nylon 6/6 (PA) Glass Fiber - Heat Stabilized
RTP Company RTP 207 K Polyarylamide (PAA), Glass Fiber
RTP Company RTP 207 MS 2 Nylon 6/6 (PA 6/6) Glass Fiber 40% - Molybdenum Disulfide 2%
RTP Company RTP 207 MS HS Nylon 6/6 (PA 6/6) Glass Fiber 40% - Molybdenum Disulfide - Heat Stable
RTP Company RTP 207 MS Nylon 6/6 (PA), Glass Fiber - Molybdenum Disulfide
RTP Company RTP 207 Nylon 6/6 (PA), Glass Fiber
RTP Company RTP 207 SI 2 Nylon 6/6 (PA 6/6) Glass Fiber 40% - Silicone 2%
RTP Company RTP 207 TFE 10 Nylon 6/6 (PA), Glass Fiber - PTFE Lubricated
RTP Company RTP 207 TFE 13 Nylon 6/6 (PA 6/6) Glass Fiber 40% - PTFE 13% - Silicone 2%
RTP Company RTP 207 TFE 13 SI 2 Nylon 6/6 (PA), Glass Fiber - PTFE Lubricated - Silicone Lubricated
RTP Company RTP 207 TFE 15 Nylon 6/6 (PA 6/6) Glass Fiber 40% - PTFE 15%
RTP Company RTP 207 TFE 5 UV Nylon 6/6 (PA 6/6) Glass Fiber 40% - PTFE 5% - UV Stable
RTP Company RTP 207 UV Nylon 6/6 (PA), Glass Fiber - UV Stabilized
RTP Company RTP 207 Z Nylon 6/6 (PA 6/6) Glass Fiber 40% - FDA Type
RTP Company RTP 207.3 Nylon 6/6 (PA 6/6) Glass Fiber 43%
RTP Company RTP 207.3 D Nylon 6/12 (PA), Glass Fiber
RTP Company RTP 207.3 HS Nylon 6/6 (PA 6/6) Glass Fiber 43% - Heat Stable
RTP Company RTP 207.3 HS SI Nylon 6/6 (PA 6/6) Glass Fiber 43% - Silicone - Heat Stable
RTP Company RTP 207.3 SI 2 Nylon 6/6 (PA 6/6) Glass Fiber 43% - Silicone 2%
RTP Company RTP 207.3 UV Nylon 6/6 (PA 6/6) Glass Fiber 43% - UV Stable
RTP Company RTP 207.3D L Nylon 6/12 (PA 6/12) Glass Fiber 43% - Lubricated
RTP Company RTP 207.3D UV Nylon 6/12 (PA 6/12) Glass Fiber 43% - UV Stable
RTP Company RTP 207.3F Nylon 12 (PA 12) Glass Fiber 43%
RTP Company RTP 207.3H HS Nylon 6/6 - High Impact (PA 6/6 HI) Glass Fiber 43% - Heat Stable - High Impact
RTP Company RTP 207A HI Nylon 6 (PA 6) Glass Fiber 40% - High Impact
RTP Company RTP 207A HS Nylon 6 (PA 6) Glass Fiber 40% - Heat Stable
RTP Company RTP 207A L Z Nylon 6 (PA 6) Glass Fiber 40% - Lubricated - FDA Type
RTP Company RTP 207A TFE 13 SI 2 HS Nylon 6 (PA 6) Glass Fiber 40% - PTFE 13% - Silicone 2% - Heat Stable
RTP Company RTP 207A TFE 15 HS Nylon 6 (PA 6) Glass Fiber 40% - PTFE 15% - Heat Stable
RTP Company RTP 207A UV Nylon 6 (PA 6) Glass Fiber 40% - UV Stable
RTP Company RTP 207B HS UV Nylon 6/10 (PA 6/10) Glass Fiber 40% - Heat Stable - UV Stable
RTP Company RTP 207D HS UV Nylon 6/12 (PA 6/12) Glass Fiber 40% - Heat Stable - UV Stable
RTP Company RTP 207D TFE 15 Nylon 6/12 (PA 6/12) Glass Fiber 40% - PTFE 15%
RTP Company RTP 207D Z Nylon 6/12 (PA 6/12) Glass Fiber 40% - FDA Type
RTP Company RTP 207E Amorphous Nylon (Am. PA) Glass Fiber 40%
RTP Company RTP 207E TFE 10 Amorphous Nylon (Am. PA) Glass Fiber 40% - PTFE 10%
RTP Company RTP 207G FR HS Nylon 4/6 (PA 4/6) Glass Fiber 40% - Flame Retardant - Heat Stable
RTP Company RTP 207G HS Nylon 4/6 (PA 4/6) Glass Fiber 40% - Heat Stable
RTP Company RTP 207H HS Nylon 6/6 - High Impact (PA 6/6 HI) Glass Fiber 40% - Heat Stable - High Impact
RTP Company RTP 208 Nylon 6/6 (PA 6/6) Glass Fiber 45%
RTP Company RTP 208 G HS L Nylon 4/6 (PA), Glass Fiber - Heat Stabilized - Lubricated - Dry As Molded
RTP Company RTP 208 K Polyarylamide (PAA), Glass Fiber
RTP Company RTP 208A Nylon 6 (PA 6) Glass Fiber 45%
RTP Company RTP 208A MS 5 Nylon 6 (PA 6) Glass Fiber 45% - Molybdenum Disulfide 5%
RTP Company RTP 208B Nylon 6/10 (PA 6/10) Glass Fiber 45%
RTP Company RTP 208G HS Nylon 4/6 (PA 4/6) Glass Fiber 45% - Heat Stable
RTP Company RTP 208G HS L Nylon 4/6 (PA 4/6) Glass Fiber 45% - Lubricated - Heat Stable
RTP Company RTP 209 A FR UV Nylon 6 (PA) Glass Fiber - Flame Retardant - UV Stabilized
RTP Company RTP 209 A Nylon 6 (PA), Glass Fiber
RTP Company RTP 209 A UV Nylon 6 (PA) Glass Fiber - UV Stabilized
RTP Company RTP 209 D Nylon 6/12 (PA), Glass Fiber
RTP Company RTP 209 G HS Nylon 4/6 (PA), Glass Fiber - Heat Stabilized - Dry As Molded
RTP Company RTP 209 HS Nylon 6/6 (PA 6/6) Glass Fiber 50% - Heat Stable
RTP Company RTP 209 K FR Polyarylamide (PAA), Glass Fiber - Flame Retardant
RTP Company RTP 209 K Polyarylamide (PAA), Glass Fiber
RTP Company RTP 209 K TFE 15 Polyarylamide (PAA), Glass Fiber - PTFE Lubricated
RTP Company RTP 209 MS 1 Nylon 6/6 (PA 6/6) Glass Fiber 50% - Molybdenum Disulfide 1%
RTP Company RTP 209 MS Nylon 6/6 (PA), Glass Fiber - Molybdenum Disulfide
RTP Company RTP 209 MS UV Nylon 6/6 (PA), Glass Fiber - Molybdenum Disulfide - UV Stabilized
RTP Company RTP 209 Nylon 6/6 (PA), Glass Fiber
RTP Company RTP 209 TFE 5 Nylon 6/6 (PA), Glass Fiber - PTFE Lubricated
RTP Company RTP 209 UV Nylon 6/6 (PA 6/6) Glass Fiber 50% - UV Stable
RTP Company RTP 209 Z Nylon 6/6 (PA 6/6) Glass Fiber 50% - FDA Type
RTP Company RTP 2099 E X 118617 B BLACK Thermoplastic Elastomer Alloy, ESD Protection - Permanently Anti-static - Polar Bondable - UV Stabilized
RTP Company RTP 2099 E X 118617 B S-886606 CHARCOAL Thermoplastic Elastomer Alloy, ESD Protection - Permanently Anti-static - Polar Bondable - UV Stabilized
RTP Company RTP 2099 X 106722 C Thermoplastic Alloy, High Gravity Compound
RTP Company RTP 2099 X 112329 Permanently Static Dissipative Masterbatch ESD Protection - Extrusion Grade
RTP Company RTP 2099 X 115375 B Bio-Based Polylactic Acid (PLA); PLA-PMMA Alloy - Impact Modified - 39% Renewable Resource Content
RTP Company RTP 2099 X 115375 C Bio-Based Polylactic Acid (PLA), PLA-PMMA Alloy - Transparent - 39% Renewable Resource Content
RTP Company RTP 2099 X 115382 C Bio-Based Polylactic Acid (PLA); PLA-HDPE Blend - 39% Renewable Resource Content
RTP Company RTP 2099 X 115387 A Biobased Polyamide (PA) Glass Fiber - 43% Bio-Content
RTP Company RTP 2099 X 115387 B Biobased Polyamide (PA) Glass Fiber - Flame Retardant - Halogen Free - 31% Bio-Content
RTP Company RTP 2099 X 115387 C Biobased Polyamide (PA) Glass Fiber - PTFE Lubricated - 34% Bio-Content
RTP Company RTP 2099 X 121216 G Polylactic Acid (PLA) Impact Modified - 80% Bio-Content
RTP Company RTP 2099 X 121235 D Bio-Based Polylactic Acid (PLA); PC-PLA Blend - 31% Renewable Resource Content
RTP Company RTP 2099 X 121236 A Biobased PLA-ABS Hybrid 40% Bio-Content
RTP Company RTP 2099 X 121240 C Biobased PLA-PC Hybrid Non Halogen Flame Retardant - 20% Bio-Content
RTP Company RTP 2099 X 121241 B Bio-Based Polylactic Acid (PLA); PC-PLA Blend - ESD Protection - Permanently Anti-static - 26% Renewable Resource Content
RTP Company RTP 2099 X 121249 A Bio-Based Polylactic Acid (PLA); Standard Nucleator - Glass Fiber - 88% Renewable Resource Content
RTP Company RTP 2099 X 121249 B Bio-Based Polylactic Acid (PLA); Standard Nucleator - Glass Fiber - 78% Renewable Resource Content
RTP Company RTP 2099 X 121249 C Bio-Based Polylactic Acid (PLA); Standard Nucleator - Glass Fiber - 68% Renewable Resource Content
RTP Company RTP 2099 X 121249 D Bio-Based Polylactic Acid (PLA); Standard Nucleator - Glass Fiber - 58% Renewable Resource Content
RTP Company RTP 2099 x 121825 E Biobased Polyamide (PA) Permanently Anti-static - ESD Protection - 31% Bio-Content
RTP Company RTP 2099 X 124789 A Bio-Based Polylactic Acid (PLA); Impact Modified - Transparent - 94% Renewable Resource Content
RTP Company RTP 2099 X 124789 B Bio-Based Polylactic Acid (PLA); Impact Modified - Transparent - 89% Renewable Resource Content
RTP Company RTP 2099 X 124789 C Bio-Based Polylactic Acid (PLA); Impact Modified - Transparent - 84% Renewable Resource Content
RTP Company RTP 2099 X 124789 D Bio-Based Polylactic Acid (PLA); Impact Modified - Transparent - 79%Renewable Resource Content
RTP Company RTP 2099 X 124790 A Bio-Based Polylactic Acid (PLA); Impact Modified - Mineral - Fast Cycle Nucleator - 78% Renewable Resource Content
RTP Company RTP 2099 X 124790 B Bio-Based Polylactic Acid (PLA); Impact Modified - Mineral - Fast-Cycle Nucleator - 68% Renewable Resource Content
RTP Company RTP 2099 X 124790 C Bio-Based Polylactic Acid (PLA); Impact Modified - Mineral - Standard Nucleator - 78% Renewable Resource Content
RTP Company RTP 2099 X 124790 D Bio-Based Polylactic Acid (PLA); Impact Modified - Mineral - Standard Nucleator - 68% Renewable Resource Content
RTP Company RTP 2099 X 124790 E Bio-Based Polylactic Acid (PLA); Impact Modified - Mineral - Fast-Cycle Nucleator - 73% Renewable Resource Content
RTP Company RTP 2099 X 124790 F Bio-Based Polylactic Acid (PLA); Impact Modified - Mineral - Fast-Cycle Nucleator - 53% Renewable Resource Content
RTP Company RTP 2099 X 126210 BLACK Bio-Based Polylactic Acid (PLA); PC-PLA Blend - 32% Renewable Resource Content - Additional 49% Post Consumer Content
RTP Company RTP 2099 X 126211 Z Bio-Based Polylactic Acid (PLA); FDA Compliant Ingredients - Impact Modified - Transparent - 89% Renewable Resource Content
RTP Company RTP 2099 X 126213 Bio-Based Polylactic Acid (PLA); PC-PLA Blend - 32% Renewable Resource Content
RTP Company RTP 2099 X 126216 A Bio-Based Polylactic Acid (PLA); Fast-Cycle Nucleator - Glass Fiber - 88% Renewable Resource Content
RTP Company RTP 2099 X 126216 B Bio-Based Polylactic Acid (PLA); Fast-Cycle Nucleator - Glass Fiber - 78% Renewable Resource Content
RTP Company RTP 2099 X 126216 C Bio-Based Polylactic Acid (PLA); Fast-Cycle Nucleator - Glass Fiber - 68% Renewable Resource Content
RTP Company RTP 2099 X 126216 D Bio-Based Polylactic Acid (PLA); Fast-Cycle Nucleator - Glass Fiber - 59% Renewable Resource Content
RTP Company RTP 2099 X 126217 Z Bio-Based Polylactic Acid (PLA); Impact Modified - FDA Compliant Ingredients - 79% Renewable Resource Content
RTP Company RTP 2099 X 126218 A Bio-Based Polylactic Acid (PLA); Impact Modified - 94% Renewable Resource Content
RTP Company RTP 2099 X 126218 B Bio-Based Polylactic Acid (PLA); Impact Modified - 89% Renewable Resource Content
RTP Company RTP 2099 X 126218 C Bio-Based Polylactic Acid (PLA); Impact Modified - 84% Renewable Resource Content
RTP Company RTP 2099 X 126218 D Bio-Based Polylactic Acid (PLA); Impact Modified - 79% Renewable Resource Content
RTP Company RTP 2099 X 127618 R Bio-Based Polylactic Acid (PLA); PC-PLA Blend - Flame Retardant - Halogen Free - 20% Renewable Resource Content
RTP Company RTP 2099 X 128018 A Polycarbonate/Polyester; Glass Fiber - Carbon Fiber - Electrically Conductive
RTP Company RTP 2099 X 128018 B PC/PBT Alloy; Glass Fiber - Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding - (Preliminary Datasheet)
RTP Company RTP 2099 X 131060 A Bio-Based Polylactic Acid (PLA), PLA ALLOY - Flame Retardant - Halogen Free - 20% Renewable Resource Content - Additional 45% Post Consumer Content
RTP Company RTP 2099 X 134503 A Polycarbonate/Polyester (PC/PBT) Glass Fiber - Flame Retardant - High Flow
RTP Company RTP 2099 X 134514 C Polycarbonate/PBT Alloy (PC/PBT), High Impact - Flame Retardant
RTP Company RTP 2099 X 134514 Polycarbonate/Polyester Flame Retardant - UV Stabilized - Chemical Resistant Alloy
RTP Company RTP 2099 X 134682 Polycarbonate/PBT Alloy; Permanently Static Dissipative - ESD Protection - Impact Modified - UV Stabilized
RTP Company RTP 2099 X 135116 U Polyester Alloy; Flame Retardant - UV Stabilized - Medical Cleaner Resistant - High Flow - UL 94 V-0
RTP Company RTP 2099 X 137399 A NS Polyester Alloy Flame Retardant - UV Stabilized - Medical Cleaner Resistant - No Subs
RTP Company RTP 2099 X 138254 A NS Polyester Alloy Medical Cleaner Resistant - UV Stabilized - No Subs
RTP Company RTP 2099 X 138757 B Permanently Static Dissipative Masterbatch; ESD Protection
RTP Company RTP 2099 X 138762 H PC/PBT Alloy Permanently Static Dissipative - ESD Protection - Impact Modified - UV Stabilized
RTP Company RTP 2099 X 138762 PC/PBT Alloy ESD Protection - Permanently Static Dissipative - Impact Modified - UV Stabilized
RTP Company RTP 2099 X 138778 Permanently Static Dissipative Masterbatch; ESD Protection
RTP Company RTP 2099 X 138791 PC/PBT; Permanently Static Dissipative - ESD Protection
RTP Company RTP 2099 X 138797 Permanently Static Dissipative Masterbatch; ESD Protection
RTP Company RTP 2099 X 141397 PC/PBT; ESD Protection - Permanently Static Dissipative - Flame Retardant - PTFE Lubricated - UV Stabilized - Preliminary Datasheet
RTP Company RTP 2099 X 141518 A Polycarbonate (PC)/Polyester; Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding - Flame Retardant - High Impact - (Preliminary Data Sheet)
RTP Company RTP 2099 X 143509 B Polyester; ESD Protection - Static Dissipative - Preliminary Datasheet
RTP Company RTP 2099 X 143976 D PC/PBT; Impact Modified - Flame Retardant - UV Stabilized
RTP Company RTP 2099 X 143988 A PC/PBT, Flame Retardant - Glass Fiber - UV Stabilized
RTP Company RTP 2099 X 144659 EG PC/PBT; ESD Protection - Electrically Conductive - Extrusion Grade
RTP Company RTP 2099 X 144671 Polycarbonate/PBT; ESD Protection - Carbon Fiber - Impact Modified - Flame Retardant - UV Stabilized - Preliminary Datasheet
RTP Company RTP 2099 X 144672 Polycarbonate/PBT Alloy (PC/PBT); ESD Protection - Carbon Fiber - Impact Modified - UV Stabilized - Preliminary Datasheet
RTP Company RTP 2099 X 144676 A Polycarbonate/PBT Alloy (PC/PBT); ESD Protection - Permanently Anti-static - Glass Fiber - Flame Retardant - Preliminary Datasheet
RTP Company RTP 2099 X 144676 C PC/PBT; ESD Protection - Permanently Anti-static - Glass Fiber - Flame Retardant - Preliminary Datasheet
RTP Company RTP 2099 X 144676 D PC/PBT; ESD Protection - Permanently Anti-static - Glass Fiber - Flame Retardant - Preliminary Datasheet
RTP Company RTP 2099 X 144679 B Permanently Static Dissipative Masterbatch; ESD Protection - Preliminary Datasheet
RTP Company RTP 2099 X 144679 Permanently Static Dissipative Masterbatch; ESD Protection
RTP Company RTP 2099 X 144682 PC/ASA; ESD Protection - Permanently Anti-static - UV Stabilized - Preliminary Datasheet
RTP Company RTP 2099 X 145616 PA6/PP; Lubricated - Preliminary Datasheet
RTP Company RTP 2099 X 146738 A Polyester; Flame Retardant - UV Stabilized - Medical Cleaner Resistant - Preliminary Datasheet
RTP Company RTP 2099 X 146986 C PC/PBT; Impact Modified - Flame Retardant - UV Stabilized - Preliminary Datasheet
RTP Company RTP 2099 X 147365 PC/PBT; ESD Protection - Permanently Static Dissipative - UV Stabilized - Preliminary Datasheet
RTP Company RTP 2099 X 149161 D PC/PBT; Flame Retardant - Impact Modified - UV Stabilized - Preliminary Datasheet
RTP Company RTP 2099 X 150724 A Nylon Alloy; Glass Fiber - Flame Retardant - Halogen Free - Preliminary Datasheet
RTP Company RTP 2099 X 153164 B S-45847 YELLOW Polycarbonate/PBT Alloy, ESD Protection - Permanently Anti-static - Impact Modified - UV Stabilized - Preliminary Datasheet
RTP Company RTP 2099 X 63578 C Polycarbonate/Polyester| (PC/PBT) Alloy, PC/PBT Alloy - UV Stabilized
RTP Company RTP 2099 X 70612 Polycarbonate/Polyester Alloy; Glass Fiber - Flame Retardant
RTP Company RTP 2099 X 90635 PC/PBT; ESD Protection - Electrically Conductive
RTP Company RTP 2099 X 91177 Thermoplastic Alloy (Alloy) Electronic Encapsulation
RTP Company RTP 209A FR UV Nylon 6 (PA 6) Glass Fiber 50% - Flame Retardant - UV Stable
RTP Company RTP 209A HI UV Nylon 6 (PA 6) Glass Fiber 50% - High Impact - UV Stable
RTP Company RTP 209A Z Nylon 6 (PA 6) Glass Fiber 50% - FDA Type
RTP Company RTP 209B Nylon 6/10 (PA 6/10) Glass Fiber 50%
RTP Company RTP 209D HS Nylon 6/12 (PA 6/12) Glass Fiber 50% - Heat Stable
RTP Company RTP 209E Amorphous Nylon (Am. PA) Glass Fiber 50%
RTP Company RTP 209F Nylon 12 (PA 12) Glass Fiber 50%
RTP Company RTP 209G HS Nylon 4/6 (PA 4/6) Glass Fiber 50% - Heat Stable
RTP Company RTP 2100 A Polyetherimide (PEI) Base Resin
RTP Company RTP 2100 AR 10 Polyetherimide (PEI) Aramid Fiber 10%
RTP Company RTP 2100 AR 15 Polyetherimide (PEI) Aramid Fiber 15%
RTP Company RTP 2100 AR 15 TFE 10 Polyetherimide (PEI) Aramid Fiber 15% - PTFE 10%
RTP Company RTP 2100 AR 15 TFE 15 Polyetherimide (PEI), Aramid Fiber - PTFE Lubricated
RTP Company RTP 2100 AR 15 TFE 15 Z Polyetherimide (PEI) Aramid Fiber 15% - PTFE 15% - FDA Type
RTP Company RTP 2100 AR 5 Polyetherimide (PEI) Aramid Fiber 5%
RTP Company RTP 2100 GB 20 Polyetherimide (PEI) Glass Bead 20%
RTP Company RTP 2100 HF Polyetherimide (PEI) High Flow
RTP Company RTP 2100 HF SI 2 Polyetherimide (PEI) Silicone 2% - High Flow
RTP Company RTP 2100 HF TFE 15 Polyetherimide (PEI) PTFE 15% - High Flow
RTP Company RTP 2100 LF Polyetherimide (PEI), Low Flow
RTP Company RTP 2100 LF TFE 10 Polyetherimide (PEI), PTFE Lubricated
RTP Company RTP 2100 LF TFE 15 Polyetherimide (PEI) PTFE 15% - Low Flow
RTP Company RTP 2100 LF Z Polyetherimide (PEI) FDA Type - Low Flow
RTP Company RTP 2100 Polyetherimide (PEI)
RTP Company RTP 2100 TFE 10 Polyetherimide (PEI), PTFE Lubricated
RTP Company RTP 2100 TFE 10 SI 2 Polyetherimide (PEI) PTFE 10% - Silicone 2%
RTP Company RTP 2100 TFE 15 Polyetherimide (PEI), PTFE Lubricated
RTP Company RTP 2100 TFE 15 Z Polyetherimide (PEI); PTFE Lubricated - FDA Compliant Ingredients
RTP Company RTP 2100 TFE 25 Polyetherimide (PEI) PTFE 25%
RTP Company RTP 2100 TFE 40 Polyetherimide (PEI), PTFE Lubricated
RTP Company RTP 2100 TFE 5 Polyetherimide (PEI) PTFE 5%
RTP Company RTP 2100 Z Polyetherimide (PEI) FDA Type
RTP Company RTP 2100.5 Polyetherimide (PEI) Glass Fiber 5%
RTP Company RTP 2101 HF Polyetherimide (PEI) Glass Fiber 10% - High Flow
RTP Company RTP 2101 LF Polyetherimide (PEI), Glass Fiber - Low Flow
RTP Company RTP 2101 Polyetherimide (PEI), Glass Fiber
RTP Company RTP 2101 TFE 10 Polyetherimide (PEI) Glass Fiber 10% - PTFE 10%
RTP Company RTP 2101 TFE 15 Polyetherimide (PEI), Glass Fiber - PTFE Lubricated - High Flow
RTP Company RTP 2101 Z Polyetherimide (PEI) Glass Fiber 10% - FDA Type
RTP Company RTP 2102 Polyetherimide (PEI), Glass Fiber
RTP Company RTP 2102 TFE 10 Polyetherimide (PEI) Glass Fiber 15% - PTFE 10%
RTP Company RTP 2102 TFE 15 Polyetherimide (PEI) Glass Fiber 15% - PTFE 15%
RTP Company RTP 2103 L Polyetherimide (PEI), Glass Fiber - Lubricated
RTP Company RTP 2103 LF Polyetherimide (PEI); Glass Fiber - Low Flow
RTP Company RTP 2103 Polyetherimide (PEI), Glass Fiber
RTP Company RTP 2103 TFE 10 Polyetherimide (PEI), Glass Fiber - PTFE Lubricated
RTP Company RTP 2103 TFE 15 Polyetherimide (PEI), Glass Fiber - PTFE Lubricated
RTP Company RTP 2103 Z Polyetherimide (PEI) Glass Fiber 20% - FDA Type
RTP Company RTP 2105 HF Polyetherimide (PEI) Glass Fiber 30% - High Flow
RTP Company RTP 2105 HF TFE 15 Polyetherimide (PEI), Glass Fiber - PTFE Lubricated
RTP Company RTP 2105 L Polyetherimide (PEI), Glass Fiber - Lubricated
RTP Company RTP 2105 LF Polyetherimide (PEI), Glass Fiber - Low Flow
RTP Company RTP 2105 Polyetherimide (PEI), Glass Fiber
RTP Company RTP 2105 TFE 10 Polyetherimide (PEI), Glass Fiber - PTFE Lubricated
RTP Company RTP 2105 TFE 15 Polyetherimide (PEI), Glass Fiber - PTFE Lubricated
RTP Company RTP 2105 TFE 15 Z Polyetherimide (PEI) Glass Fiber 30% - PTFE 15% - FDA Type
RTP Company RTP 2105 TFE 5 Polyetherimide (PEI) Glass Fiber 30% - PTFE 5%
RTP Company RTP 2105 Z Polyetherimide (PEI), Glass Fiber - FDA Compliant Ingredients
RTP Company RTP 2105.3 HF Polyetherimide (PEI) Glass Fiber 33% - High Flow
RTP Company RTP 2107 LF Polyetherimide (PEI), Glass Fiber - Low Flow
RTP Company RTP 2107 Polyetherimide (PEI), Glass Fiber
RTP Company RTP 2107 Z Polyetherimide (PEI) Glass Fiber 40% - FDA Type
RTP Company RTP 2109 Polyetherimide (PEI) Glass Fiber 50%
RTP Company RTP 211 A Nylon 6 (PA), Glass Fiber
RTP Company RTP 211 G HS Nylon 4/6 (PA), Glass Fiber - Heat Stabilized - Dry As Molded
RTP Company RTP 211 HS Nylon 6/6 (PA 6/6) Glass Fiber 60% - Heat Stable
RTP Company RTP 211 K Polyarylamide (PAA), Glass Fiber
RTP Company RTP 211 L Nylon 6/6 (PA 6/6) Glass Fiber 60% - Lubricated
RTP Company RTP 211 Nylon 6/6 (PA), Glass Fiber
RTP Company RTP 211D Nylon 6/12 (PA 6/12) Glass Fiber 60%
RTP Company RTP 211G HS Nylon 4/6 (PA 4/6) Glass Fiber 60% - Heat Stable
RTP Company RTP 2181 HEC HF Polyetherimide (PEI), Nickel-Coated Carbon Fiber - Electrically Conductive - EMI/RFI Shielding - High Flow - Easy Molding
RTP Company RTP 2181 HEC Polyetherimide (PEI) Nickel-Coated Carbon Fiber - Electrically Conductive - EMI/RFI Shielding
RTP Company RTP 2181 HF TFE 15 Polyetherimide (PEI), Carbon Fiber - PTFE Lubricated
RTP Company RTP 2181 Polyetherimide (PEI) Carbon Fiber
RTP Company RTP 2181 TFE 10 Polyetherimide (PEI); Carbon Fiber - PTFE Lubricated
RTP Company RTP 2181 TFE 15 SI 2 Polyetherimide (PEI) Carbon Fiber - PTFE Lubricated - Silicone Lubricated
RTP Company RTP 2181 TFE 5 Polyetherimide (PEI), Carbon Fiber - PTFE Lubricated
RTP Company RTP 2182 Polyetherimide (PEI) Carbon Fiber 15%
RTP Company RTP 2183 HEC Polyetherimide (PEI), Nickel-Coated Carbon Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company RTP 2183 HF Polyetherimide (PEI), Carbon Fiber
RTP Company RTP 2183 LF Polyetherimide (PEI) Carbon Fiber 20% - Low Flow
RTP Company RTP 2183 Polyetherimide (PEI); Carbon Fiber
RTP Company RTP 2183 TFE 10 Polyetherimide (PEI); Carbon Fiber - PTFE Lubricated
RTP Company RTP 2184 HEC Polyetherimide (PEI), Nickel-Coated Carbon Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company RTP 2184 L Polyetherimide (PEI) Carbon Fiber - Easy Molding
RTP Company RTP 2184 Polyetherimide (PEI) Carbon Fiber
RTP Company RTP 2184 TFE 15 Polyetherimide (PEI) Carbon Fiber 25% - PTFE 15%
RTP Company RTP 2185 HEC Polyetherimide (PEI); Nickel-Coated Carbon Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company RTP 2185 Polyetherimide (PEI); Carbon Fiber
RTP Company RTP 2185 TFE 13 SI 2 Polyetherimide (PEI) Carbon Fiber 30% - PTFE 13% - Silicone 2%
RTP Company RTP 2185 TFE 15 Polyetherimide (PEI), Carbon Fiber - PTFE Lubricated
RTP Company RTP 2185 TFE 5 Polyetherimide (PEI) Carbon Fiber 30% - PTFE 5%
RTP Company RTP 2187 HEC Polyetherimide (PEI), Nickel-Coated Carbon Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company RTP 2187 L Polyetherimide (PEI) Carbon Fiber 40% - Lubricated
RTP Company RTP 2187 Polyetherimide (PEI); Carbon Fiber
RTP Company RTP 2199 X 115079 A Polyetherimide (PEI), Carbon Nanotube - ESD Protection
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.