System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Drill Down to All Materials Data Sheets
This series of pages is an inefficient set of links to all data sheets in MatWeb. We have several search tools, listed above, that give you more efficient methods to reach the information that you need.
Replacing...
Quantum PBT
Quantum PEEK
Quantum PEEK 30% Carbon Filled
Quantum PEEK 30% Glass Fiber Filled
Quantum PEI - Ultem®
Quantum PEI - Ultem® 30% Glass Fiber Filled
Quantum PET
Quantum Polycarbonate
Quantum Polycarbonate 20% Glass Fiber Filled
Quantum Polysulfone
Quantum PPS
Quantum PPSU
Quantum PVDF
Quartz (SiO
2
)
Quartz Sand Soil, Dry
Quartz Sand Soil, Wet; 4-23 wt.% Water
Quartzite
QuesTek® Innovations Ferrium® C61™ Case-hardened Gear Steel with Ultrahigh-strength Core
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications
RA 85 H Austenitic Stainless Steel, UNS S30615 (Composition Spec)
RA-330HC Iron-Nickel Alloy
RA-333 Nickel Alloy (UNS N06333)
Radiata Pine Wood
Radici Heraflex ® E 2517 1000 NT Thermoplastic Polyester Elastomer
Radici Heraflex ® E 3918 1000 NAT Thermoplastic Polyester Elastomer
Radici Heraflex ® E 4718 1000 NAT Thermoplastic Polyester Elastomer
Radici Heraflex ® E 6521 1000 NAT Thermoplastic Polyester Elastomer
Radici Heraflex ® E 7722 1000 NAT Thermoplastic Polyester Elastomer
Radici Heraflex ® E MTE5505UK 100NT Thermoplastic Polyester Elastomer
Radici Heraflex ® E MTE6305UK 100NT Thermoplastic Polyester Elastomer
Radici Heraflex® A 35-13-40 TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 40-11-91 TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 55 11 I HW TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 55 42 I HW2E TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 55 I RKT TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 57-41-90 TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 60 31 I HS1 TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 65 31 I HW TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 65-21-20 UV TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 70-21-22 TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 70-21-22 UV TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 70-22-90 HG TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 75-21-60 TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 80-21-94 TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 80-42-90 G TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 90-11-44 UV TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® A 90-21-90 TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® B 35D 11 I SL 250 Styrenic Thermoplastic Elastomer SBS
Radici Heraflex® B 60 11 I HP Styrenic Thermoplastic Elastomer SBS
Radici Heraflex® B 80 31 I HP Styrenic Thermoplastic Elastomer SBS
Radici Heraflex® E 3918 TPC-ET Thermoplastic Elastomer
Radici Heraflex® E 4718 TPC-ET Thermoplastic Elastomer
Radici Heraflex® E 5620 TPC-ET Thermoplastic Elastomer
Radici Heraflex® E 6521 TPC-ET Thermoplastic Elastomer
Radici Heraflex® E 7722 TPC-ET Thermoplastic Elastomer
Radici Heraflex® HA 60-22-60 TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® HP 40-21-60 TPS-SEBS Thermoplastic Elastomer
Radici Heraflex® P 40D 11 I HF 1530 Modified Polypropylene
Radici Heraflex® P 40D 21 I HF Modified Polypropylene
Radici Heraflex® P 51D 11 I RB T 270 Modified Polypropylene
Radici Heraflex® P 55D 11 I HF 330 Modified Polypropylene
Radici Heraflex® P46D 11 I RB T 200 Modified Polypropylene
Radici Heraform® R 1300 Acetal Copolymer
Radici Heraform® R 3000 Acetal Copolymer
Radici Heraform® R 350 Acetal Copolymer
Radici Heraform® R 900 Acetal Copolymer
Radici Heramid ® A NER GF030/1K Polyamide 66
Radici Heramid ® A NER MP/1K Polyamide 66
Radici Radiflam® A AE (cond.) Nylon 66
Radici Radiflam® A AE (dry) Nylon 66
Radici Radiflam® A FR (cond.) Nylon 66
Radici Radiflam® A FR 100 NT Polyamide 66
Radici RADIFLAM® A FRX 328 BK Nylon 66, Flame Retardant, Conditioned
Radici RADIFLAM® A FRX 328 BK Nylon 66, Flame Retardant, Dry
Radici Radiflam® A RV250 AF 375 BK Polyamide 66
Radici RADIFLAM® A RV250 HF 100 NT Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant, Conditioned
Radici RADIFLAM® A RV250 HF 100 NT Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant, Dry
Radici Radiflam® A RV250 HF 333 BK Polyamide 66
Radici Radiflam® A RV250AF (cond.) Nylon 66-25GF
Radici Radiflam® A RV250AF (dry) Nylon 66-25GF
Radici Radiflam® A RV250FR (cond.) Nylon 66-25GF
Radici Radiflam® A RV250FR (dry) Nylon 66-25GF
Radici Radiflam® A RV300AE (cond.) Nylon 66-30GF
Radici Radiflam® A RV300AF (cond.) Nylon 66-30GF
Radici Radiflam® A RV300AF (dry) Nylon 66-30GF
Radici Radiflam® A RV350AF (cond.) Nylon 66-35GF
Radici Radiflam® A RV500 AF 821 BR Polyamide 66
Radici Radiflam® AESTUS T2 RV300 HF 100 NT Polyphthalamide
Radici RADIFLAM® AESTUS T2 RV300 HF 333 BK Nylon 66, 30% Glass Fiber Reinforced, Flame Retardant, Conditioned
Radici RADIFLAM® AESTUS T2 RV300 HF 333 BK Nylon 66, 30% Glass Fiber Reinforced, Flame Retardant, Dry
Radici Radiflam® AFR (dry) Nylon 66
Radici Radiflam® ARV300 AE (dry) Nylon 66
Radici RADIFLAM® ARV300 AF 830 BR Nylon 66, 30% Glass Fiber Reinforced, Flame Retardant, Conditioned
Radici RADIFLAM® ARV300 AF 830 BR Nylon 66, 30% Glass Fiber Reinforced, Flame Retardant, Dry
Radici Radiflam® ARV350 AF (dry) Nylon 66
Radici Radiflam® B RV 300 AE Polybutylene Terephthalate
Radici Radiflam® B RV250AE Polybutylene Terephthalate - 25% Glass fiber reinforced
Radici RADIFLAM® B RV300K AE 135 NT PBT, 30% Glass Fiber Reinforced, Flame Retardant
Radici Radiflam® B RV300K AE 375 BK Polybutylene Terephthalate
Radici Radiflam® BN100 AE Polybutylene Terephthalate
Radici Radiflam® BRV300 AE Polybutylene Terephthalate
Radici Radiflam® S AE (cond.) Nylon 6
Radici Radiflam® S AE (dry) Nylon 6
Radici Radiflam® S FR (cond.) Nylon 6
Radici RADIFLAM® S FR 100 NT PBT, Flame Retardant, Conditioned
Radici RADIFLAM® S FR 100 NT PBT, Flame Retardant, Dry
Radici Radiflam® S FR 137 NAT Polyamide 6
Radici Radiflam® S RV250FR (cond.) Nylon 6
Radici Radiflam® S RV250FR (dry) Nylon 6
Radici Radiflam® S RV300 HF 148 NT Polyamide 6
Radici RADIFLAM® S RV300 HF 333 BK Nylon 6, 30% Glass Fiber Reinforced, Flame Retardant, Conditioned
Radici RADIFLAM® S RV300 HF 333 BK Nylon 6, 30% Glass Fiber Reinforced, Flame Retardant, Dry
Radici Radiflam® S RV300AE (cond.) Nylon 6
Radici Radiflam® S RV300AE (dry) Nylon 6
Radici Radiflam® SFR (dry) Nylon 6
Radici Radilene® R 30 IE 0 3036 B Low Density Polyethylene
Radici Radilene® R 70 IE 0 2060 C High Density Polyethylene
Radici Radilene® R 70 IE 5058 B High Density Polyethylene
Radici Radilene® R 70 IF 0 4058 A High Density Polyethylene
Radici Radilon® A 35E 990 (cond.) Nylon 66
Radici Radilon® A 35E 990 (dry) Nylon 66
Radici Radilon® A 38 (cond.) Nylon 66
Radici Radilon® A 38 (dry) Nylon 66
Radici Radilon® A 42 (cond.) Nylon 66
Radici Radilon® A 42 (dry) Nylon 66
Radici Radilon® A 42K 100 M NT Polyamide 66
Radici Radilon® A 50HSKB 870 M BR Polyamide 66
Radici Radilon® A CF200 333 BK Polyamide 66
Radici Radilon® A CF300K 333BK Polyamide 66
Radici Radilon® A CF350 (cond.) Nylon 66
Radici Radilon® A CF350 (dry) Nylon 66
Radici Radilon® A CP300K (cond.) Nylon 66
Radici Radilon® A CP300K 333BK Polyamide 66
Radici Radilon® A CP300K 333BK Polyamide 66
Radici Radilon® A CP400 (cond.) Nylon 66
Radici Radilon® A CP400 (dry) Nylon 66
Radici Radilon® A CV300LK (cond.) Nylon 66
Radici Radilon® A CV300LK (dry) Nylon 66
Radici Radilon® A ECP3808 (cond.) Nylon 66
Radici Radilon® A ECP3808 (dry) Nylon 66
Radici Radilon® A ERV1906LK (cond.) Nylon 66
Radici Radilon® A ERV3012 (cond.) Nylon 66
Radici Radilon® A ERV3012 (dry) Nylon 66
Radici Radilon® A ESL128 100 NT Polyamide 66
Radici Radilon® A GV H0 30P Nylon 66-GF30
Radici Radilon® A HS (cond.) Nylon 66
Radici Radilon® A HS 164 NT Polyamide 66
Radici Radilon® A HSK (cond.) Nylon 66
Radici Radilon® A HSK (dry) Nylon 66
Radici RADILON® A HSK 164 NT Nylon 66, Heat Stabilized, Conditioned
Radici RADILON® A HSK 164 NT Nylon 66, Heat Stabilized, Dry
Radici Radilon® A HSX (dry) Nylon 66
Radici Radilon® A HSX 100 NT Polyamide 66
Radici Radilon® A HSX88 (cond.) Nylon 66
Radici RADILON® A HSX88 100NT Nylon 66, Conditioned
Radici RADILON® A HSX88 100NT Nylon 66, Dry
Radici Radilon® A LRV600W 333 BK Polyamide 66
Radici Radilon® A LX14080 (cond.) Nylon 66
Radici Radilon® A RCF3505 (cond.) Nylon 66
Radici Radilon® A RCF3505 (dry) Nylon 66
Radici Radilon® A RCV3015 RKC Nylon 66-GF30
Radici RADILON® A RCW4015W 3733 BK Nylon 66, 40% Glass/Mineral Reinforced, Conditioned
Radici RADILON® A RCW4015W 3733 BK Nylon 66, 40% Glass/Mineral Reinforced, Dry
Radici Radilon® A RFL4530 100 NT Polyamide 66
Radici Radilon® A RV150 (cond.) Nylon 66
Radici Radilon® A RV150 (dry) Nylon 66
Radici Radilon® A RV150W 333 BK Polyamide 66
Radici Radilon® A RV200 (cond.) Nylon 66
Radici Radilon® A RV200 (dry) Nylon 66
Radici RADILON® A RV200L 100NT Nylon 66, 20% Glass Fiber Reinforced, Conditioned
Radici RADILON® A RV200L 100NT Nylon 66, 20% Glass Fiber Reinforced, Dry
Radici Radilon® A RV250 (cond.) Nylon 66
Radici Radilon® A RV250 (dry) Nylon 66
Radici Radilon® A RV300 (cond.) Nylon 66
Radici Radilon® A RV300 990 (cond.) Nylon 66
Radici Radilon® A RV300 990 (dry) Nylon 66
Radici RADILON® A RV300 990 GY Nylon 66, 30% Glass Fiber Reinforced, Conditioned
Radici RADILON® A RV300 990 GY Nylon 66, 30% Glass Fiber Reinforced, Dry
Radici RADILON® A RV300FC 100 NT Nylon 66, 30% Glass Fiber Reinforced, Conditioned
Radici RADILON® A RV300FC 100 NT Nylon 66, 30% Glass Fiber Reinforced, Dry
Radici Radilon® A RV300HRG 3900 BK Polyamide 66
Radici RADILON® A RV300K 1700 NT Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized, Conditioned
Radici RADILON® A RV300K 1700 NT Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized, Dry
Radici Radilon® A RV300R (cond.) Nylon 66
Radici Radilon® A RV300R (dry) Nylon 66
Radici Radilon® A RV300RG 3900 BK Polyamide 66
Radici Radilon® A RV300RKC (cond.) Nylon 66
Radici Radilon® A RV300RKC 106NT Polyamide 66
Radici RADILON® A RV300RKC 306 BK Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized, Conditioned
Radici RADILON® A RV300RKC 306 BK Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized, Dry
Radici RADILON® A RV300RKC2 106 NT Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized, Conditioned
Radici RADILON® A RV300RKC2 106 NT Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized, Dry
Radici RADILON® A RV300RKC2 306 BK Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized, Conditioned
Radici RADILON® A RV300RKC2 306 BK Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized, Dry
Radici RADILON® A RV300W 333 BK Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized, Conditioned
Radici RADILON® A RV300W 333 BK Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized, Dry
Radici Radilon® A RV330 (cond.) Nylon 66
Radici Radilon® A RV330 (dry) Nylon 66
Radici Radilon® A RV350 (cond) Nylon 66
Radici Radilon® A RV350 (dry) Nylon 66
Radici RADILON® A RV350 100 NT Nylon 66, 35% Glass Fiber Reinforced, Conditioned
Radici RADILON® A RV350 100 NT Nylon 66, 35% Glass Fiber Reinforced, Dry
Radici RADILON® A RV350 AF 375 BK Nylon 66, 35% Glass Fiber Reinforced, Conditioned
Radici RADILON® A RV350 AF 375 BK Nylon 66, 35% Glass Fiber Reinforced, Dry
Radici Radilon® A RV350HHR 3800 BK Polyamide 66
Radici RADILON® A RV350RW 339 BK Nylon 66, 35% Glass Fiber Reinforced, Heat Stabilized, Conditioned
Radici RADILON® A RV350RW 339 BK Nylon 66, 35% Glass Fiber Reinforced, Heat Stabilized, Dry
Radici Radilon® A RV350USR 333 BK Polyamide 66
Radici Radilon® A RV350W 333 BK Polyamide 66
Radici RADILON® A RV350X2N 333 BK Nylon 66, 35% Glass Fiber Reinforced, Conditioned
Radici RADILON® A RV350X2N 333 BK Nylon 66, 35% Glass Fiber Reinforced, Dry
Radici Radilon® A RV400 (cond.) Nylon 66
Radici Radilon® A RV400 (dry) Nylon 66
Radici Radilon® A RV500 (cond.) Nylon 66
Radici Radilon® A RV500 (dry) Nylon 66
Radici RADILON® A RV500 100 NT Nylon 66, 50% Glass Fiber Reinforced, Conditioned
Radici RADILON® A RV500 100 NT Nylon 66, 50% Glass Fiber Reinforced, Dry
Radici Radilon® A RV500HHR 3800 BK Polyamide 66
Radici RADILON® A RV500RKC 306 BK Nylon 66, 50% Glass Fiber Reinforced, Heat Stabilized, Conditioned
Radici RADILON® A RV500RKC 306 BK Nylon 66, 50% Glass Fiber Reinforced, Heat Stabilized, Dry
Radici RADILON® A RV500RKC2 306 BK Nylon 66, 50% Glass Fiber Reinforced, Heat Stabilized, Conditioned
Radici RADILON® A RV500RKC2 306 BK Nylon 66, 50% Glass Fiber Reinforced, Heat Stabilized, Dry
Radici Radilon® A RV500RW 339 BK Polyamide 66
Radici Radilon® A USX200 100 NAT Polyamide 66
Radici Radilon® A USZ200 100 NT Polyamide 66
Radici RADILON® ADLINE CS CF10 HP BK Nylon 6/66, 10% Carbon Fiber Reinforced, Conditioned
Radici RADILON® ADLINE CS CF10 HP BK Nylon 6/66, 10% Carbon Fiber Reinforced, Dry
Radici RADILON® ADLINE CS Nylon 6/66, Conditioned
Radici RADILON® ADLINE CS Nylon 6/66, Dry
Radici Radilon® AERV1906 LK (dry) Nylon 66
Radici Radilon® Aestus T1 RV300RKC 306 BK Polyphthalamide
Radici Radilon® Aestus T1 RV330RG 3900 BK Polyphthalamide
Radici Radilon® Aestus T1 RV400RKC 306 BK Polyphthalamide
Radici Radilon® Aestus T2 RV350W 333 BK Polyphthalamide
Radici Radilon® AHS (dry) Nylon 66
Radici Radilon® AHSX88 (dry) Nylon 66
Radici Radilon® ALX14080 (dry) Nylon 66
Radici Radilon® ARV300 (dry) Nylon 66
Radici Radilon® ARV300 RKC (dry) Nylon 66
Radici Radilon® AUSX200 (dry) Nylon 66
Radici Radilon® CA HS (cond.) Nylon 66/6
Radici Radilon® CA RV200UK 3110 BK Polyamide 66/6
Radici Radilon® CA RV300L (cond.) Nylon 66/6
Radici Radilon® CAHS (dry) Copolyamide 66/6
Radici Radilon® CARV300 L (dry) Copolyamide 66/6
Radici Radilon® CS 35FL (cond.) Nylon 6/66
Radici Radilon® CS 35FL (dry) Nylon 6/66
Radici Radilon® CS 38FL (cond.) Nylon 6/66
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.