MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Vyncolit X6151 Novolac Phenolic
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral/Glass Filled

Material Notes: Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Highest impact, high strain to failure, glycol resistant.

USES: Water pumps and water pump impellers without metal insert bushes. Intake manifolds.

Information provided by Vyncolit, a Sumitomo Bakelite Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 g/cc0.0217 lb/in³Powder Density; ISO 60
Density 1.55 g/cc0.0560 lb/in³Relative Density; ISO 1183
Linear Mold Shrinkage 0.0035 cm/cm0.0035 in/inInjection Molding; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psiISO 527
Elongation at Break 0.90 %0.90 %Tensile; ISO 527
Tensile Modulus 11.0 GPa1600 ksiISO 527
Flexural Strength 160 MPa23200 psiAt Rupture; ISO 178
Flexural Modulus 10.0 GPa1450 ksiISO 178
Flexural Strain at Break 1.65 %1.65 %ISO 178
Compressive Strength 220 MPa31900 psiISO 604
Charpy Impact Unnotched 1.20 J/cm²5.71 ft-lb/in²ISO 179
Charpy Impact, Notched 0.350 J/cm²1.67 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 30.0 kV/mm762 kV/inIEC 243
Comparative Tracking Index 175 V175 VIEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature 20.0 °C
13.9 µin/in-°F
@Temperature 68.0 °F
TMA
CTE, linear, Transverse to Flow 45.0 µm/m-°C
@Temperature 20.0 °C
25.0 µin/in-°F
@Temperature 68.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FISO 75 Af
Flammability, UL94  V-1
@Thickness 1.60 mm
V-1
@Thickness 0.0630 in
 V-0
@Thickness 4.00 mm
V-0
@Thickness 0.157 in
Shrinkage 0.10 %0.10 %Post Shrinkage; ISO 2577
 
Descriptive Properties
ColorBlack
ISO typePF 2 C3
Main FillerGlass Fiber & Mineral
Molding MethodCompression, transfer, injection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Vyncolit X7012 Glass Fiber Reinforced Novolac Phenolic
Vyncolit X7255 Glass Fiber Reinforced Novolac Phenolic
Vyncolit BXE7665 Glass Filled Phenolic Molding Compound
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound
Vyncolit X655 Novolac Phenolic

PVYNC010 / 72218

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.