Novolac resin based, glass fiber, mineral and graphite filled. Grade with superior stiffness, high dimensional stability and excellent tribological properties. Good chemical resistance against several fuels at elevated temperatures. Used for fuel pump housings.Information provided by Sumitomo Bakelite North America, Inc. |