MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Encom Polymers EnPure F040GF PC, 40% Glass Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 40% Glass Filled; Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: Appearance: Black, Natural or Colors

Processing Methods: Injection Molding, Profile Extrusion

Applications: Electrical / Electronic Applications

Information provided by EnCom Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/ccASTM D792
Filler Content 40 %40 %
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm
@Thickness 3.20 mm
0.0010 - 0.0020 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 155 MPa22500 psiASTM D638
Tensile Strength, Yield 159 MPa23100 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 186 MPa27000 psiASTM D790
Flexural Modulus 9.655 GPa1400 ksiASTM D790
Izod Impact, Notched 0.800 J/cm1.50 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C306 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 146 °C295 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 288 - 310 °C550 - 590 °F
Middle Barrel Temperature 299 - 321 °C570 - 610 °F
Front Barrel Temperature 310 - 332 °C590 - 630 °F
Nozzle Temperature 304 - 327 °C580 - 620 °F
Melt Temperature 310 - 332 °C590 - 630 °F
Mold Temperature 82.2 - 116 °C180 - 240 °F
Drying Temperature 93.3 - 121 °C200 - 250 °F
Dry Time 4.00 hour4.00 hour
 <= 7.00 hour<= 7.00 hour
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
Shot Size 40 - 75 %40 - 75 %
Vent Depth 0.00381 - 0.00762 cm0.00150 - 0.00300 in
Screw Speed 25 - 75 rpm25 - 75 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENCOM104 / 266118

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.