MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Outokumpu 4724 High Temperature Ferritic Stainless Steel
Categories: Metal; Ferrous Metal; Ferritic; Stainless Steel

Material Notes: Truly stainless high temperature grade with 13% chromium. Not critical in terms of embrittlement.

Applications: Mostly used in high temperature applications with sulphurous atmospheres and/or low tensile loads such as for installations within:

  • Chemical industry (drums)
  • Power industry (coal burners)
  • Metalworking industry (heat treatment boxes)
  • Furnace technology (walls, doors)

Available in hot rolled plate (Quarto) form.

Key Words: EN 1.4724
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.60 g/cc0.275 lb/in³RT
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 192192RT; EN 10003-1
Tensile Strength, Ultimate 515 MPa74700 psiOutokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Tensile Strength, Yield  340 MPa
@Strain 0.2 %
49300 psi
@Strain 0.2 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 370 MPa
@Strain 1 %
53700 psi
@Strain 1 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Elongation at Break 30 %30 %Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000920 ohm-cm0.0000920 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.2 µm/m-°C
@Temperature 600 °C
6.78 µin/in-°F
@Temperature 1110 °F
Specific Heat Capacity 0.440 J/g-°C0.105 BTU/lb-°FRT
Thermal Conductivity 15.7 W/m-K109 BTU-in/hr-ft²-°FRT
 22.3 W/m-K
@Temperature 500 °C
155 BTU-in/hr-ft²-°F
@Temperature 932 °F
Maximum Service Temperature, Air 850 °C1560 °FDry Air
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 800 - 850 °C1470 - 1560 °FCooling: forced air or water
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.70 %0.70 %
Carbon, C 0.12 %0.12 %
Chromium, Cr 13 %13 %
Iron, Fe 86.18 %86.18 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AK Steel 15 Cr-Cb® ULTRA FORM® Ferritic Stainless steel
Outokumpu 4713 High Temperature Ferritic Stainless Steel
Aluminum 5086-H112
AISI 321 Cast Stainless Steel, ASTM A276 Hot Formed
316 Stainless Steel, annealed sheet

NOUTOK37 / 18752

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.