MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ITW Spraycore® SC VELR 4000 Vinyl Ester Mold Building Resin
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes: SC VELR 4000 is a DCPD/Vinyl Ester laminating resin. This product is a low shrink resin that rapidly wets out the fiber glass reinforcement and cures uniformly with a low exothermic. MEKP catalyst is not included. Product Features: formulated to cure uniformly with low exothermic, offers low shrinkage upon curing, helps reduce fiber glass print, increases part rigidity without adding thickness. Product benefits: helps to speed up and simplify production, reduces manufacturing costs, helps extend part life. Preferred red dye catalyst: HP-90, DHP-9, MEKP 925.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 - 1.10 g/cc0.0381 - 0.0398 lb/in³Application density
Viscosity 450 - 650 cP450 - 650 cPRVF #2 @ 20rpm
 
Chemical PropertiesMetricEnglishComments
Styrene Content 32 %32 %
 
Processing PropertiesMetricEnglishComments
Gel Time 4.00 - 10.0 min4.00 - 10.0 minGel to Peak
 15.0 - 25.0 min15.0 - 25.0 min
 
Descriptive Properties
ColorAmber
Peak Exotherm325 to 375°F100g mass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ITW Spraycore® SC 4700 Tooling Resin

PITWS9057 / 239567

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.