MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Ceramacast™ 515 High Temperature Potting & Casting Aluminum Oxide
Categories: Ceramic; Oxide; Silicon Oxide; Potting/Casting Ceramic

Material Notes: Fine Grain, High Strength Potting Compound. Binder is K2O-SiO2

Cure:
Step 1. Dry for 16–24 hours at room temperature.
Step 2. Bake at 200ºF for 1–4 hours.
Step 3. Bake at 250ºF for 1–4 hours.
Step 4. Bake at 350ºF for 1 hour.
Step 5. Final cure at 500ºF for 1 hour.

Vendors: Aremco’s Ceramacast casting and potting compounds represent the most expansive line of products based on aluminum oxide, aluminum nitride, magnesium oxide, silicon dioxide, silicon carbide, zirconium oxide, and zirconium silicate for applications to 3000°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³
Porosity <= 2.0 %<= 2.0 %
pH 11 - 1211 - 12
Viscosity 10000 cP10000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 75.8 MPa11000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+9 ohm-cm1.00e+9 ohm-cm
Dielectric Strength 9.84 kV/mm250 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.10 µm/m-°C
@Temperature 20.0 °C
4.50 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 1650 °C3000 °F
Shrinkage <= 1 %
@Temperature 538 °C
<= 1 %
@Temperature 1000 °F
 
Processing PropertiesMetricEnglishComments
Dry Time 20 - 24.0 hour20 - 24.0 hourAir dry prior to cure
Cure Time 300 - 420 min5.00 - 7.00 hoursee notes
Pot Life 120 - 180 min120 - 180 min
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Acid ResistanceGoodattacked by HF
Alkali ResistanceGood
BinderK2-SiO2
ColorWhite
Mix Ratio100:12-14powder:water
Moisture ResistanceGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CAREM46m / 256033

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.