MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Hexcel® HexPly® F650 Bismaleimide Resin with Quartz 581 reinforcement
Categories: Polymer; Thermoset; Bismaleimide (BMI)

Material Notes: Laminate Physicals: 47.2% Fiber volume, 38.4% Resin content, 0.5% Voids

Information provided by HexCel

Key Words: BMI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.31
@Temperature 24.0 °C
3.31
@Temperature 75.2 °F
 3.33
@Temperature 149 °C
3.33
@Temperature 300 °F
 3.34
@Frequency 9.375e+9 Hz,
Temperature 232 °C
3.34
@Frequency 9.375e+9 Hz,
Temperature 450 °F
Dielectric Loss Index  0.0030
@Temperature 24.0 °C
0.0030
@Temperature 75.2 °F
 0.0040
@Temperature 149 °C
0.0040
@Temperature 300 °F
 0.0050
@Frequency 9.375e+9 Hz,
Temperature 232 °C
0.0050
@Frequency 9.375e+9 Hz,
Temperature 450 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay MTM® 110 series Ester Matrix Resin
Solvay CYCOM® 5250-4 BMI Prepreg Neat Resin
Solvay CORFIL® 5250-4 Potting Compound
Hexcel® HexPly® F650 Bismaleimide Resin
Solvay CYCOM® 5250-4 BMI Prepreg System with IM-7 Carbon Fiber

PHEXC005 / 98475

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.