MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oxford Polymers C-Acetal -30GF-Natural Acetal Copolymer, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 30% Glass Fiber Reinforced

Material Notes: Product Description: Glass Fiber (30% Reinforced), Co-polymer Acetal, Injection Molding Grade

Processing and Delivery Form: Pellets and Injection Molding

Additives: Glass Fiber

Special Characteristics: Excellent creep resistance

Information provided by Oxford Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.58 g/cc0.0571 lb/in³ASTM D792
Water Absorption at Saturation 0.45 %0.45 %ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 3.17 mm
0.0040 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 125 MPa18200 psiASTM D638
Elongation at Break 1.5 %1.5 %ASTM D638
Flexural Modulus 7.24 GPa1050 ksiASTM D790
Izod Impact, Notched 0.854 J/cm
@Thickness 3.17 mm
1.60 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C170 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 177 - 199 °C350 - 390 °F
Middle Barrel Temperature 182 - 204 °C360 - 400 °F
Front Barrel Temperature 188 - 210 °C370 - 410 °F
Nozzle Temperature 188 - 210 °C370 - 410 °F
Melt Temperature 182 - 218 °C360 - 425 °F
Mold Temperature 79.4 - 107 °C175 - 225 °F
Drying Temperature 93.3 °C200 °F
Dry Time 2.00 hour2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
Polyram RamTal PM3007G6 Acetal, 30% Glass Fiber
RTP Company RTP 4207 Thermoplastic Polyimide (TPI), Glass Fiber - UL94 V-0
RTP Company RTP 4285 Thermoplastic Polyimide (TPI) Carbon Fiber

POXF005 / 178435

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.