MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips 66 SynXPA® H-500 H Lubricant H-500
Categories: Fluid; Lubricant; Synthetic Ether Base

Material Notes: Description: Conoco SynXPA H Lubricant is a premium-quality synthetic-polyolester lubricant that offers protection for heavily loaded and partially opened open gears, such as those in ball mills, shovels, kilns and draglines. It is also useful for wire ropes, shovel boom sticks and slow moving bearings. It is inherently biodegradable (up to 90 percent biodegradable, as per CEC, OECD testing) and nontoxic (As per acute mammalian toxicity studies.). SynXPA H Lubricant can be applied to the surface through most automatic lubricators or through automated delivery lines and an air assisted sprayer. Pressure-lubrication bins, lines and pumps need not be purged unless they are plugged by residual asphaltic materials. SynXPA H Lubricant meets the performance requirements of the American Gear Manufacturers Association (AGMA) 251.02 Specification for high-viscosity-grade, extreme-pressure gear lubricants. SynXPA H Lubricant offers high film strength and film thickness. It spreads out and coats surfaces evenly for better distribution of load. It reduces the gear surface temperatures and minimizes the temperature gradient across the gear face, which typically is associated with slightly misaligned gear sets. Polyolesters have great affinity for metals. As such, SynXPA H Lubricant bonds to gear surfaces and provides exceptional shock loading protection at startups and in situations where the equipment may be idle for extended periods of time.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Kinematic Viscosity at 40°C (104°F) 11000 cSt11000 cSt
Kinematic Viscosity at 100°C (212°F) 500 cSt500 cSt
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Load Wear Index 7070
Four Ball Extreme Pressure, Weld Load 315 kg695 lb (mass)
Four Ball Wear 0.310 mm0.0122 in
Penetration 265 - 295265 - 295ASTM D-217
Timken Test 34000 g75.0 lb
 
Thermal PropertiesMetricEnglishComments
Flash Point 191 °C375 °F
 
Descriptive Properties
ColorBrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON184 / 75221

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.