MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECATEC PA12 CF50 T200 CP/IP/OS V01 natural Nylon 12, 50% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Carbon Fiber Filled

Material Notes:
  • very good abrasion resistance
  • very good mechanical strength
  • low moisture absorption
Target Industries:
  • automotive industry
  • mechanical engineering
  • oil and gas industry
  • safety engineering
  • sporting goods

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³
Filler Content 50 %50 %Fiber volume
 50.0 %50.0 %Fiber Volume
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 37.0 MPa5370 psiISO 527-4
Modulus of Elasticity 53.0 GPa7690 ksiISO 527-4
Flexural Strength 637 MPa92400 psiISO 14125
Flexural Modulus 52.5 GPa7610 ksiISO 14125
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 3.00 µm/m-°C1.67 µin/in-°F
CTE, linear, Transverse to Flow 3.00 µm/m-°C1.67 µin/in-°F
Melting Point 180 °C356 °FDIN EN ISO 11357
Maximum Service Temperature, Air 110 °C230 °Flong term
 150 °C302 °Fshort term
Glass Transition Temp, Tg 37.0 °C98.6 °FDIN EN ISO 11357
 
Processing PropertiesMetricEnglishComments
Drying Temperature 80.0 °C176 °F
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hour
 
Descriptive Properties
Colornatural
General material information0.22 mmply thickness (consolidated)
 1000 mmMaterial widths
 1270 mmMaterial widths
 200 g/m²Fiber areal weight
 327 g/m²Areal weight finished product
 carbon HT 3kFiber type
 twill 2/2Fiber architecture
Resin weight content (%)38.4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8236 / 319164

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.