MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Ticuni™ Mac-Ticuni™-WM Braze Alloy
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy; Titanium Alloy

Material Notes: A high-purity Active Brazing Filler in composite form containing titanium, copper and nickel, developed for direct application to ceramic surfaces.

Applications:

  • Aerospace components
  • Medical equipment components
  • Vacuum tubes
  • Wave guide and Klystron assemblies

information provided by Morgan Advanced Materials

Key Words: Braze Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.26 g/cc0.190 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point 910 - 960 °C1670 - 1760 °F
Solidus 910 °C1670 °F
Liquidus 960 °C1760 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 960 - 1100 °C1760 - 2010 °FBrazing Temperature
 
Component Elements PropertiesMetricEnglishComments
Cadmium, Cd <= 0.0010 %<= 0.0010 %
Copper, Cu 15 %15 %nominal
Lead, Pb <= 0.0020 %<= 0.0020 %
Nickel, Ni 15 %15 %nominal
Phosphorus, P <= 0.0020 %<= 0.0020 %
Titanium, Ti 70 %70 %nominal
Zinc, Zn <= 0.0010 %<= 0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Johnson Matthey Tri-flo™ 950 Titanium Brazing Filler Metal
Morgan Advanced Ceramics Nicoro™ Mac-Nicoro™-WM Braze Alloy
Morgan Advanced Ceramics Nioro™ ABA Mac-Nioro™ABA-WM Braze Alloy
Morgan Advanced Ceramics Nioro™ Mac-Nioro™-WM Braze Alloy
Morgan Advanced Ceramics Mac-35 Au/65 Cu-WM Braze Alloy

CMORF8003 / 203480

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.