MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil EVA 2009.PM Low Density Polyethylene (LDPE), Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Product Description: ExxonMobil™ EVA 2009.PM is a 8.7 wt% vinyl acetate copolymer film resin. Films made from EVA 2009.PM resin exhibit superior impact strength and heat sealability.

Availability: Latin America and North America

Additive:  antiblock: no; slip: no; thermal stabilizer: yes. 

Applications:  meat packaging, primal meat bags.  Forms: pellets.

Information provided by ExxonMobil.

Key Words: LDPE LD 319.PM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D1505
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 6.34 MPa920 psiASTM D882
Film Tensile Strength at Yield, TD 5.86 MPa850 psiASTM D882
Film Elongation at Break, MD 330 %330 %ASTM D882
Film Elongation at Break, TD 660 %660 %ASTM D882
Puncture Energy 3.05 J2.25 ft-lbExxonMobil Method
Elmendorf Tear Strength MD 120 g120 gASTM D1922
Elmendorf Tear Strength TD 80 g80 gASTM D1922
Dart Drop Test 360 g0.794 lbASTM D1709A
Film Tensile Strength at Break, MD 31.0 MPa4500 psiASTM D882
Film Tensile Strength at Break, TD 27.6 MPa4000 psiASTM D882
1% Secant Modulus, MD 96.5 MPa14000 psiASTM D882
1% Secant Modulus, TD 110 MPa16000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 97.8 °C208 °FPeak; ExxonMobil Method
Vicat Softening Point 77.2 °C171 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 1.9 %1.9 %ASTM D1003
Gloss 85 %85 %@ 45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEX98877 / 238259

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.