MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elix Polymers ELIX ABS L3FR Acrylonitrile Butadiene Styrene (ABS), Flame Retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Flame retardant ABS

ISO Shortname: ABS 1, MGF, 085-25-09-25

Information provided by Elix Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Melt Flow 50 g/10 min
@Load 10.0 kg,
Temperature 220 °C
50 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 105 MPa15200 psiISO 2039-1
Tensile Strength, Yield 42.0 MPa6090 psi50 mm/min; ISO 527-1,-2
Tensile Modulus 2.40 GPa348 ksi1 mm/min; ISO 527-1,-2
Izod Impact, Notched (ISO)  4.00 kJ/m²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 8.00 kJ/m²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  40.0 kJ/m²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 60.0 kJ/m²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant  3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
IEC 60250
 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor  0.070
@Frequency 100 Hz
0.070
@Frequency 100 Hz
IEC 60250
 0.080
@Frequency 1e+6 Hz
0.080
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 450 V450 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C192 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FISO 75-1,-2
Vicat Softening Point  85.0 °C
@Load 5.10 kg
185 °F
@Load 11.2 lb
50°C/h; ISO 306
 88.0 °C
@Load 5.10 kg
190 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Glow Wire Flammability Index 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 °C446 °FInjection molding; ISO 294
Mold Temperature 70.0 °C158 °FInjection molding; ISO 294
Injection Velocity 200 mm/sec7.87 in/secInjection molding; ISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Beijing Chemical Industry KAIFA® GL3100 ABS Flame-Retardant Grade
A. Schulman Diamond ABS VP-12
Elix Polymers ELIX ABS M3FR Acrylonitrile Butadiene Styrene (ABS), Flame Retardant
Beijing Chemical Industry KAIFA® GL3300 ABS Flame-Retardant Grade
Chi Mei Polylac® PA-765 ABS - Flame Retardant

PELIX028 / 183343

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.