MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC CYCOLAC™ FR15U ABS (Europe)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94V-0/5VA rated. Elevated UL RTI rating.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Water Absorption 1.0 %1.0 %23°C/sat; ISO 62
Moisture Absorption 0.200 %0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inSABIC method
Melt Flow  7.0 g/10 min
@Load 5.00 kg,
Temperature 220 °C
7.0 g/10 min
@Load 11.0 lb,
Temperature 428 °F
ISO 1133
 40 g/10 min
@Load 10.0 kg,
Temperature 220 °C
40 g/10 min
@Load 22.0 lb,
Temperature 428 °F
cm³/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 41.0 MPa5950 psi50 mm/min; ISO 527
Elongation at Break 22 %22 %50 mm/min; ISO 527
Tensile Modulus 2.21 GPa321 ksi1mm/min; ISO 527
Flexural Yield Strength 63.0 MPa9140 psi2 mm/min; ISO 178
Flexural Modulus 2.26 GPa328 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²5.71 ft-lb/in²80*10*4; ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Dielectric Strength 20.0 kV/mm
@Thickness 3.20 mm
508 kV/in
@Thickness 0.126 in
in oil; IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FISO 8302
Vicat Softening Point 92.0 °C198 °FRate B/50; ISO 306
UL RTI, Electrical 60.0 °C140 °FUL 746B
UL RTI, Mechanical with Impact 60.0 °C140 °FUL 746B
UL RTI, Mechanical without Impact 60.0 °C140 °FUL 746B
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 5VA
@Thickness 2.80 mm
5VA
@Thickness 0.110 in
UL 94
Oxygen Index 26 %26 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature
Nozzle Temperature 190 - 220 °C374 - 428 °FInjection Molding
Zone 1 180 - 210 °C356 - 410 °F
Zone 2 195 - 225 °C383 - 437 °F
Zone 3 195 - 225 °C383 - 437 °F
Melt Temperature 200 - 230 °C392 - 446 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 80.0 - 85.0 °C176 - 185 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Moisture Content 0.10 %0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10032 / 243499

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.