MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Polyplastics TOPAS® 6013EC-01 COC
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: Tough, non-transparent grade.

TOPAS is an amorphous copolymer based on the polymerization of ethylene and nor-bornene using metallocene catalysts. Its property profile can be varied over a wide range by adjusting the chemical structure during polymerization.

Information provided by Polyplastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 36.0 MPa5220 psi5 mm/min; ISO 527-2/1A
Elongation at Break 30 %30 %5mm/min; ISO 527-2/1A
Flexural Strength 62.0 MPa8990 psiISO 178
Flexural Modulus 1.80 GPa261 ksiISO 178
Charpy Impact, Notched 3.60 J/cm²17.1 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.27
@Frequency 1e+9 Hz
2.27
@Frequency 1e+9 Hz
IEC 60250
Dissipation Factor 0.00060
@Frequency 1e+9 Hz
0.00060
@Frequency 1e+9 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FISO-75-1.2
Flammability, UL94 HBHB
 
Descriptive Properties
ISO Marking Code>COC<ISO 11469; JIS K6999
UL Yellow Card FileE31940

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastics TOPAS® 5013F-04 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 6013L-17 COC
Polyplastics TOPAS® 9506F-500 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 8007F-600 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 9506F-04 COC

PPOLPL126c / 191495

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.