MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sylvania SA901C Molybdenum Thermal Spray Powder
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: General Description

SA901 is a blend of SA101 molybdenum plasma spray powder plus an atomized nickel alloy powder. This blend exhibits excellent flow characteristics. The particle size distribution can be modified to satisfy specific customer requirements.

Applications

  • Piston rings for internal combustion engines

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.40 - 3.00 g/cc0.0867 - 0.108 lb/in³
Particle Mesh Size 100 Mesh100 Mesh100% smaller
 170 - 325 Mesh170 - 325 Mesh82%
 325 Mesh325 Mesh15% smaller
 
Component Elements PropertiesMetricEnglishComments
Boron, B 1.0 %1.0 %
Carbon, C 0.80 %0.80 %
Chromium, Cr 4.0 %4.0 %
Iron, Fe 1.0 %1.0 %
Molybdenum, Mo 75 %75 %
Nickel, Ni 17.2 %17.2 %
Silicon, Si 1.0 %1.0 %
 
Descriptive Properties
Hall Flow, seconds/50g20-30ASTM B213

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
414 Stainless Steel, tempered at 508°C
California Fine Wire Stablohm 710 Nickel Chromium Resistance Wire
ATI Allvac® Allcorr® UNS N06110 Nickel Superalloy
AISI Type S21904 (Alloy 21-6-9) Stainless Steel, sheet and strip 0% cold reduction, stress relieved at 480°C (900°F) for 1 hour
AISI Type 430F(Se) Stainless Steel annealed bar

CSYLV04 / 2303

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.