MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Polyplastics TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC)
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface making it an excellent choice for healthcare and other high-tech products. Lower leachables and extractables of TOPAS COC preserve food and drug stability and quality. Analytical results are more accurate with TOPAS COC in contact with sensitive chemistries.

Key applications and attributes:

  • Drug delivery: Low leachables & extractables, low water transmission
  • Prefilled syringes, vials, cartridges: Non-ionic, does not promote adsorption like glass
  • Bottles and tubes: Minimally reactive, EtO and irradiation sterilizable
  • Surgical instruments: Chemically resistant to alcohol, acetone, and acrylates
  • IV containers and components: Transparent, withstands EtO and gamma sterilization
  • Labware:Temperature resistance, clarity and purity
  • Optics: Clarity, low birefringence, low moisture sensitivity
  • Electronics: Low dielectric constant, thermoplastic
  • Food packaging: Not manufactured with BPA, phthalates, or halogens
  • Healthcare and food: Broad regulatory approval

Information provided by Polyplastics USA, which merged with TOPAS Advanced Polymers in 2018.

Key Words: Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Oxygen Permeability 977 cm3 mil/(m2 day atm)63.0 cm3 mil/(100 in2 day atm)1 mil nominal thickness
Water Vapor Permeability 3.70 g mil/ (m2 day)0.239 g mil/ (100 in2 day)1 mil nominal thickness
Density 1.02 g/cc0.0368 lb/in³ISO 1183
Water Absorption at Saturation 0.010 %
@Temperature 23.0 °C
0.010 %
@Temperature 73.4 °F
ISO 62
Melt Flow 29.4 g/10 min
@Load 2.16 kg,
Temperature 260 °C
29.4 g/10 min
@Load 4.76 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 63.0 MPa9140 psi50mm/min; ISO 527-2/1A
Elongation at Yield 4.5 %4.5 %50mm/min; ISO 527-2/1A
Tensile Modulus 2.60 GPa377 ksi1mm/min; ISO 527-2/1A
Charpy Impact Unnotched 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.260 J/cm²
@Temperature 23.0 °C
1.24 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmIEC 60093
Dielectric Constant 2.35
@Frequency 1000 - 10000 Hz
2.35
@Frequency 1000 - 10000 Hz
IEC 60250
Comparative Tracking Index >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FISO 75-1,-2
Vicat Softening Point 80.0 °C176 °FB50 (50°C/h 50N); ISO 306
Glass Transition Temp, Tg 78.0 °C172 °F10°C/min; ISO 11357-1,-2,-3
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.531.53ISO 489
Transmission, Visible 91 %91 %ISO 13468-2
 
Processing PropertiesMetricEnglishComments
Feed Temperature <= 60.0 °C<= 140 °F
Nozzle Temperature 220 - 250 °C428 - 482 °F
Zone 1 190 - 220 °C374 - 428 °F
Zone 2 200 - 230 °C392 - 446 °F
Zone 3 210 - 240 °C410 - 464 °F
Zone 4 220 - 250 °C428 - 482 °F
Mold Temperature 40.0 - 70.0 °C104 - 158 °F
Injection Velocity 50.0 - 150 mm/sec1.97 - 5.91 in/secModerate to Fast
Injection Pressure 50.0 - 110 MPa7250 - 16000 psiSpecific
Hold Pressure 30.0 - 60.0 MPa4350 - 8700 psiSpecific
Back Pressure <= 15.0 MPa<= 2180 psiSpecific
Screw Speed 50 - 200 rpm50 - 200 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 2458 Polycarbonate, Injection Grade
Avient Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
BASF Elastollan® C 70 A HPM TPUR
BASF Elastollan® C-70AW Polyester Type Polyurethane Elastomer

POTOPAS12 / 82415

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.