MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman BMC 620M Mineral Filled, Glass Fiber Reinforced Polyester Compound
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: BMC 620M molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by high impact strength, good moldability excellent overall electrical properties and flame resistance.

Typical applications include phase separators circuit breaker housings, and applications requiring the properties of Military specification Mil-M-14G Type MAI-60.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.86 g/cc1.86 g/cc
Water Absorption 0.13 %0.13 %24 hours, 23°C
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm0.0015 - 0.0025 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 30 - 4030 - 40
Tensile Strength, Ultimate 55.2 - 68.9 MPa8000 - 10000 psi
Flexural Strength 138 - 165 MPa20000 - 24000 psi
Compressive Strength 165 - 193 MPa24000 - 28000 psi
Izod Impact, Notched 4.81 - 5.87 J/cm9.00 - 11.0 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.2
@Frequency 60 Hz
5.2
@Frequency 60 Hz
Dielectric Strength 14.2 kV/mm360 kV/inShort Time
Dissipation Factor 0.020
@Frequency 60 Hz
0.020
@Frequency 60 Hz
Arc Resistance 185 sec185 sec
Comparative Tracking Index >= 500 V>= 500 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °F
Flammability, UL94  V-0
@Thickness 6.35 mm
V-0
@Thickness 0.250 in
 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Mold Temperature 138 - 166 °C280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman BMC 620 Mineral Filled, Glass Fiber Reinforced Polyester Compound
Haysite 270FRII Polyester BMC, Glass Reinforced
A. Schulman BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester
A. Schulman BMC 680 Mineral Filled, Glass Fiber Reinforced Polyester Compound
A. Schulman BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound

PBMC023 / 27206

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.