MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Polimersan Plastics POLITEF® (PTFE) with 25% Carbon
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Carbon Fiber Filled

Material Notes:
  • Electrical Conductivity
  • Increase At Corrosion Resistance
  • Increase In Deformation Strength Against Load
  • Decrease In Thermal Expansion
  • High Resistance Against Acids
  • Ease of Mechanical Processing
  • Stretching
  • Resistance Against Stroke
  • Increase In Thermal Conductivity

Information provided by Polimersan Polimer Kimya San.Tic.Ltd.Sti.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.10 - 2.20 g/cc2.10 - 2.20 g/ccASTM D1457-18
Deformation 5.0 - 6.0 %5.0 - 6.0 %230°C, 1 day, 140 kg/cm^2; ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 60 - 6760 - 67ASTM D2240
Tensile Strength, Yield 16.2 - 16.7 MPa2350 - 2420 psiASTM D1708
Elongation at Break 155 - 165 %155 - 165 %ASTM D1708
Izod Impact, Notched 0.834 J/cm1.56 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 13.0 - 19.0 kV/mm330 - 483 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 - 110 µm/m-°C
@Temperature 20.0 °C
44.4 - 61.1 µin/in-°F
@Temperature 68.0 °F
ASTM E831
Thermal Conductivity 0.98788 W/m-K6.8448 BTU-in/hr-ft²-°FASTM C177
 
Descriptive Properties
Corrosion30 - 40 cc-dak/kg-ms25 - 1000°C
Kinding Temperature630°C, ASTM D1929

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carlisle 201LD Carbon-Carbon Composite
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced
Murtfeldt Murflor® Polytetrafluoroethylene
Murtfeldt Murflor® Polytetrafluoroethylene, 25% Carbon
Eurotec® Tecomid® NA40 CR10 BK111 PA6.6, 10% carbon fiber reinforced, black

PPOLIM02 / 56968

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.