MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Cerama-Dip™ 540 High Temperature Specialty Ceramic-Inorganic Coating
Categories: Ceramic; Oxide; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Ceramic-inorganic coating. Medium viscosity, green pigmented, phosphate-bonded, high strength, electrical insulation coating for applications to 3000ºF (1650ºC).

Vendors: Aremco’s high temperature coatings and sealers are formulated using ceramic, glass and silicone technologies for a broad range of electrical insulation applications. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.22 g/cc2.22 g/cc
Solids Content 48.9 %48.9 %by volume
 75 %75 %by weight
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Viscosity 15000 - 25000 cP15000 - 25000 cPBrooksfield LV Viscometer
Thickness 25.4 microns1.00 milrecommended dry film thickness
 52.1 microns2.05 milestimated wet film thickness
Storage Temperature 12.8 - 29.4 °C55.0 - 85.0 °F
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 2.76 kV/mm70.0 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1650 °C3000 °F
 
Processing PropertiesMetricEnglishComments
Dry Time 1 hour1 hourTouch
 1 hour1 hourHandling
Cure Time >= 60.0 min>= 1.00 hourAir Set prior to curing
 180 - 300 min3.00 - 5.00 hour1-2 hr at 200°F followed by 1-2 hr at 350°F, then 1 hr at 500°F
Shelf Life 6.0 Month
@Temperature 12.8 - 29.4 °C
6.0 Month
@Temperature 55.0 - 85.0 °F
 
Descriptive Properties
Application Temperature50 - 90°F
ColorGreen
Dry Film Coverage ft2/gal784at 1 mil
Thinner540-T

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CAREM39m / 256035

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.