MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Xenia Materials XECARB® 20-C15-SL Nylon 11, 15% Carbon Fiber Reinforced Lightweight Composite
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11 + Carbon Fiber

Material Notes: XECARB® SL thermoplastic composites are used for special applications in drones, UAV’s and cobot industries, as well as applications in sport systems.

Information provided by Xenia Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/inSim. ISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/inSim. ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 145 MPa21000 psi5 mm/min; ISO 527
Elongation at Break 4.2 %4.2 %5 mm/min; ISO 527
Tensile Modulus 10.7 GPa1550 ksi1 mm/min; ISO 527
Flexural Yield Strength 185 MPa
@Strain 3.5 %
26800 psi
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 8.60 GPa1250 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  11.0 kJ/m²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 180
 14.0 kJ/m²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
50 % RH; ISO 180
Izod Impact, Unnotched (ISO)  59.0 kJ/m²
@Temperature -30.0 °C
28.1 ft-lb/in²
@Temperature -22.0 °F
ISO 180
 62.0 kJ/m²
@Temperature 23.0 °C
29.5 ft-lb/in²
@Temperature 73.4 °F
50 % RH; ISO 180
 
Processing PropertiesMetricEnglishComments
Melt Temperature 225 - 240 °C437 - 464 °F
Mold Temperature 50.0 °C122 °F
Drying Temperature 80.0 - 100 °C176 - 212 °Fdesiccant dryer
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hourdesiccant dryer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PXENIA900 / 268476

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.