MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Materion SupremEX® 225CA Aluminum - Silicon Carbide Metal Matrix Composite, T4, HIPed Billet
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy

Material Notes: A high-quality aluminum alloy (2124A) reinforced with 25 vol.% silicon carbide particles which produces a metal matrix composite (MMC). 225CA is manufactured via a powder metallurgy route using a mechanical alloying process to ensure a homogeneous distribution of reinforcement. This provides a refined grain structure and enhanced mechanical properties. The 225CA MMC is heat treatable, offering high strength and elastic modulus for structural applications. 225CA is available in a variety of shapes including billet and forgings.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.88 g/cc0.104 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 572 MPa83000 psi
Tensile Strength, Yield 455 MPa
@Strain 0.200 %
66000 psi
@Strain 0.200 %
Elongation at Break 1.50 %1.50 %
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.3000.300
Shear Modulus 44.0 GPa6380 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.4 µm/m-°C9.10 µin/in-°F
Specific Heat Capacity 0.829 J/g-°C0.198 BTU/lb-°F
Thermal Conductivity 156 W/m-K1080 BTU-in/hr-ft²-°F
Solidus 548 °C1020 °F
 
Descriptive Properties
Specific Stiffness39 GPa/g/cm3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NBB9113l / 323547

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.