MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Momentive Performance Materials TSE3331 Dark Gray Thermally Conductive Potting/Encapsulating Compound
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Elastomer, for Thermal Management

Material Notes: Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depths. Typical uses: Power assemblies with thermal dissipation.

Data provided by the manufacturer, GE Silicones.

GE Silicones became a part of Momentive Performance Materials in 2006.

Key Words: RTV Silicones; R.T.V. Silicones
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³
Viscosity 3500 cP
@Temperature 25.0 °C
3500 cP
@Temperature 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060
Tensile Strength, Ultimate 3.24 MPa470 psi
Elongation at Break 50 %50 %
Tear Strength 3.40 kN/m19.4 pliDie B
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cm
Dielectric Constant 3.3
@Frequency 1000 Hz
3.3
@Frequency 1000 Hz
Dielectric Strength 20.0 kV/mm
@Thickness 1.91 mm
508 kV/in
@Thickness 0.0750 in
Dissipation Factor 0.0030
@Frequency 1000 Hz
0.0030
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 170 µm/m-°C
@Temperature 20.0 °C
94.4 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.630 W/m-K4.37 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °FContinuous useful temperature.
Minimum Service Temperature, Air -60.0 °C-76.0 °FContinuous useful temperature.
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °FCure time 8 hours.
Pot Life 540 min
@Temperature 25.0 °C
540 min
@Temperature 77.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Cure Resin
Tra-Con Tra-Bond 2151 Thermally Conductive Electrically Insulating Compound
Master Bond MasterSil 156 Two Part, Low Viscosity Silicone
Momentive Performance Materials RTV31 Red Extreme High Temperature Potting/Encapsulating Compound
Momentive Performance Materials XE20-A7013U Heat Cured Rubber - Thermal Conductive

PZZGE988 / 40542

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.