MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ASI® Pipe Sealer TORQUE 20RC and TORQUE 20RCHH Anaerobic Methacrylate Ester Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: TORQUE 20RC and TORQUE 20RCHH are anaerobic resins that are the best method for retaining, locking, and sealing a wide range of metal parts. Even in the tightest fitting assemblies voids are presents which allows for movement and potential loosening of the parts. TORQUE 20RC and 20RCHH form a tough, durable resin, that fills all these voids, creating a unitized assembly that is completely resistant to shock, vibration, and extremely harsh environmental conditions. These materials cure in the absence of air and in the present of metal. They are suited for retaining cylindrical assemblies providing shock and vibration resistance.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc
@Temperature 25.0 °C
1.10 g/cc
@Temperature 77.0 °F
uncured
Brookfield Viscosity  8000 cP
@Temperature 20.0 °C
8000 cP
@Temperature 68.0 °F
Uncured. Spindle 5- 20 rpm. 20RC
 12000 cP
@Temperature 20.0 °C
12000 cP
@Temperature 68.0 °F
Uncured. Spindle 5- 20 rpm. 20RCHV
Storage Temperature 8.00 - 28.0 °C46.4 - 82.4 °Funcured
 
Mechanical PropertiesMetricEnglishComments
Shear Strength >= 13.8 MPa>= 2000 psiISO 10123
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.0000800 µm/m-°C0.0000444 µin/in-°Fcured; ASTM D696
Specific Heat Capacity 0.300 J/g-°C0.0717 BTU/lb-°Fcured
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°Fcured; ASTM C177
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flash Point >= 100 °C>= 212 °Funcured
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 20.0 °C
12.0 Month
@Temperature 68.0 °F
uncured
 
Descriptive Properties
Chemical ClassMethacrylate Ester
Color / appearanceGreen liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASINC9199 / 233565

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.