MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Quantum Composites HTC-9500 55% E-Glass Fiber Reinforced Bismaleimide SMC, High Temperature Composite
Categories: Polymer; Thermoset; Bismaleimide (BMI); Composite SMC

Material Notes: HTC-9500 (127-51-6) is an E-Glass Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristics providing greatly extended service temperature range versus epoxy compounds for compression molding applications.

  • Form = Rolled Sheet
  • Color = Natural
  • Glass Fiber Content = 55% nominal

A. Schulman has acquired Quantum Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.82 g/cc1.82 g/ccASTM D792
Linear Mold Shrinkage 0.0015 cm/cm0.0015 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 196 MPa28400 psiASTM D638
Tensile Modulus 33.8 GPa4900 ksiASTM D638
Flexural Strength 648 MPa94000 psiASTM D790
Flexural Modulus 27.6 GPa4000 ksiASTM D790
 
Processing PropertiesMetricEnglishComments
Shelf Life  1.00 Month
@Temperature 4.44 °C
1.00 Month
@Temperature 40.0 °F
 6.00 Month
@Temperature -12.2 °C
6.00 Month
@Temperature 10.0 °F
 
Descriptive Properties
Fiber Length (in)1E-Glass, nominal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay CYCOM® 5250-4 BMI Prepreg System with IM-7 Carbon Fiber
Quantum Composites HTC-9593 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite
Solvay CORFIL® 5250-4 Potting Compound
Solvay DURATOOL® 450 BMI Tooling Prepreg
Solvay FM® 475 BMI Syntactic Core

PCOQB918 / 139286

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.