MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Exxtra™ Soft EMA5024 Molding Ethylene Methyl Acrylate, Molding Grade
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Molding Grade

Material Notes: Exxtra™ Soft EMA5024 an ethylene methyl acrylate copolymer that can be used in specialty bonding applications and as a toughener for engineering polymers. It can be processed at temperatures as low as 200°F (93°C) and as high as 600°F (315°C).

Availability: Latin America; North America

Additive: Antiblock: No; Slip: No; Thermal Stabilizer: Yes

Applications: Compatibilizer; Engineering Polymer Toughener; Low Temperature Sealant Compounds; Masterbatch Base Resin

Information provided by ExxonMobil.

Key Words: Optema™ TC 221 Molding
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ASTM D1505
Methyl Acrylate Content 24 %24 %ExxonMobil Method
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 82
@Time 15.0 sec
82
@Time 0.00417 hour
ASTM D2240
Hardness, Shore D 24
@Time 15.0 sec
24
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 6.69 MPa970 psiASTM D638
Elongation at Break >= 600 %>= 600 %ASTM D638
Flexural Modulus, 1% Secant 26.9 MPa3900 psiASTM D790
Dart Drop, Total Energy  17.6 J
@Temperature 22.8 °C
13.0 ft-lb
@Temperature 73.0 °F
Instrumented; ASTM D3763
 23.0 J
@Temperature -40.0 °C
17.0 ft-lb
@Temperature -40.0 °F
Instrumented; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Melting Point 72.8 °C163 °FPeak; ExxonMobil Method
Vicat Softening Point 45.0 °C113 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEX98903 / 238285

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.