MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Helium, He
Categories: Fluid; Pure Element

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.000164 g/cc0.00000592 lb/in³Gas
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 4.0026024.0026021995
Atomic Number 22
Critical Temperature -267.96 °C-450.33 °F
Critical Molar Volume 57.0 cm³/mol3.48 in³/mol
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 5.193 J/g-°C1.241 BTU/lb-°F
Thermal Conductivity  0.0755 W/m-K
@Pressure 0.000 MPa,
Temperature -173 °C
0.524 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature -280 °F
gas; low pressure limiting value
 0.1193 W/m-K
@Pressure 0.000 MPa,
Temperature -73.1 °C
0.8279 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature -99.7 °F
gas; low pressure limiting value
 0.1567 W/m-K
@Pressure 0.000 MPa,
Temperature 26.9 °C
1.087 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 80.3 °F
gas; low pressure limiting value
 0.1906 W/m-K
@Pressure 0.000 MPa,
Temperature 127 °C
1.323 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 260 °F
gas; low pressure limiting value
 0.2223 W/m-K
@Pressure 0.000 MPa,
Temperature 227 °C
1.543 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 440 °F
gas; low pressure limiting value
 0.2524 W/m-K
@Pressure 0.000 MPa,
Temperature 327 °C
1.752 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 620 °F
gas; low pressure limiting value
Boiling Point -268.93 °C-452.07 °F
Heat of Formation 0.000 kJ/mol0.000 kJ/molGas
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.02451
@Temperature -269 °C,
Wavelength 546 nm
1.02451
@Temperature -452 °F,
Wavelength 546 nm
 
Component Elements PropertiesMetricEnglishComments
Helium, He 100 %100 %
 
Descriptive Properties
AppearanceColorless Gas
CAS Number7440-59-7

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Argon, Ar
Hydrogen, H2
Nitrogen, N2
Oxygen (O2)
Neon, Ne

AMEHe / 42

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.