Single-part castable ceramic exhibiting high strength and thermal conductivity. Cure: Step 1. Dry for 8 hours minimum at room temperature. Step 2. Bake at 200 ºF for 2–4 hours. Step 3. Final cure at 250 ºF for 3 hours. Step 4. Final cure at 450 ºF for 30–60 minutes if using HLB-1 Hydrophobic Liquid Binder. |
Aremco’s ceramic and graphite adhesives are ideal for bonding, potting and sealing probes, sensors, halogen lamps, igniters, power resistors, cartridge heaters, filters, fiberoptics, honeycombs, and graphite structures to 3200°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |