MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wellman PermaClear™ HP806 (0.84 IV) PET  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: PermaClear® HP806 is a TPA-based polyethylene terephthalate resin made especially for use in packaging applications. It is a solid-stated copolymer resin with an intrinsic viscosity 0.84 IV. PermaClear® HP806 may be used in contact with food in full compliance with the Federal Food, Drug, and Cosmetic Act and applicable food additive regulations including 21 CFR Section 177.1630.

Information provided by DAK Americas. Wellman is a subsidiary of DAK Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.897 g/cc0.0324 lb/in³Nominal
Viscosity Test 82 - 86 cm³/g0.82 - 0.86 dl/gIntrinsic; BD-61201-1
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 240 °C>= 464 °FBD-61305
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Chip Size0.24-0.44 gm/20 chipsBD-61223
Color-4.5-0b*, BD-6600
 77-81L*, BD-6600
Compounds<2 ppmAcetaldehyde, Measured on chip, BD-61301

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Eastman Vitiva PC715 PET
CENTROPLAST CENTROLYTE FG Polyethylene terephthalate, Food Grade
Overview of materials for Polycarbonate/PET Polyester Blend
Wellman AquaClear® Ti844 PET

PDAKA007 / 147982

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.