MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Thermx® CGT33 NC010 PCT
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced

Material Notes: Thermx® CGT33 NC010 is a 30% glass fiber reinforced, toughened polycyclohexylenedimethylene terephthalate resin for injection molding.

Celenese acquired the Thermx product line from DuPont in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³ISO 1183
Filler Content 30 %30 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psiISO 527
Elongation at Break 2.8 %2.8 %ISO 527
Tensile Modulus 8.40 GPa
@Temperature 23.0 °C
1220 ksi
@Temperature 73.4 °F
ISO 527
Flexural Strength 180 MPa26100 psiISO 178
Flexural Modulus 7.60 GPa1100 ksiISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 285 °C545 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75-1/-2
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL94
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
IEC 60695-11-10
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
UL94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 300 °C572 °FOptimum
 295 - 310 °C563 - 590 °F
Mold Temperature 100 °C212 °FOptimum
 80.0 - 120 °C176 - 248 °F
Drying Temperature 95.0 °C203 °F
Dry Time 4 - 6 hour4 - 6 hourDehumidified Dryer
Moisture Content <= 0.030 %<= 0.030 %
 
Descriptive Properties
ColorNatural
Drying RecommendedYes
FillerGlass Reinforced
FormsPellets
GenericPCT
Part Marking Code>PCT-IGF30<ISO 11469
Polymer FamilyPolyester
Polymer TypePCT
Processing MethodInjection Molding
Product CategoryElectrical Resins
 Glass Reinforced Resins
 Toughened Resins
Region AvailableAmericas
 Asia/Pacific
 Europe
Resin IdentificationPCT-IGF30ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Celanese Thermx® CGT33 BK010T PCT
Celanese Thermx® CGT33 PCT, 30% Specialty

PDTA7738 / 89697

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.