MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Techmer ES Electrablend® PA6 04001 FR MB Glass/Stainless Steel Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled; Nylon 6, Stainless Steel Filled

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Glass/Stainless Steel Fiber

Additive: Lubricated

Features: Electromagnetic Shielding (EMI), Lubricated, Flame Retardant and Radio Frequency Shielding (RFI)

Appearance: Blue

Information provided by TP Composites, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³ASTM D792
Water Absorption 1.0 %
@Time 86400 sec
1.0 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 3.17 mm
0.0020 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 117117ASTM D785
Tensile Strength, Yield 131 MPa19000 psiASTM D638
Elongation at Break 3.5 %3.5 %ASTM D638
Flexural Strength 186 MPa27000 psiASTM D790
Flexural Modulus 7.58 GPa1100 ksiASTM D790
Izod Impact, Notched 0.694 J/cm
@Thickness 3.17 mm
1.30 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.0 - 10 ohm-cm1.0 - 10 ohm-cmASTM D257
Surface Resistance 10 - 1000 ohm10 - 1000 ohmASTM D257
Static Decay <= 2.0 sec<= 2.0 secFTMS 101B
Shielding Effectiveness 50 dB50 dBASTM D4935
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 54.0 µm/m-°C30.0 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FUnannealed; ASTM D648
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company EMI 261 A Nylon 6 (PA), Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
RTP Company EMI 262 Nylon 6/6 (PA), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 261 Nylon 6/6 (PA), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 261 H Impact-Modified Nylon 6/6 (PA), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 260.6 Nylon 6/6 (PA), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection

PTPC0987 / 136925

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.