MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lotte Advanced Materials Starex® MP-0160RD Metal Plating Grade ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Plating Grade

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Water Absorption 0.20 %0.20 %ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D955
Melt Flow 2.4 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.4 g/10 min
@Load 11.0 lb,
Temperature 392 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength, Yield 44.1 MPa
@Thickness 3.17 mm
6400 psi
@Thickness 0.125 in
ASTM D638
Flexural Strength 64.8 MPa
@Thickness 3.17 mm
9400 psi
@Thickness 0.125 in
ASTM D790
Flexural Modulus 2.34 GPa
@Thickness 3.17 mm
340 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 2.56 J/cm
@Thickness 3.17 mm
4.80 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 86.1 °C
@Thickness 6.35 mm
187 °F
@Thickness 0.250 in
Unannealed; ASTM D648
Vicat Softening Point 98.0 °C208 °FUnannealed; ISO R 306
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Optical PropertiesMetricEnglishComments
Gloss 96 %96 %ASTM D523
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 190 - 210 °C374 - 410 °F
Middle Barrel Temperature 200 - 220 °C392 - 428 °F
Front Barrel Temperature 210 - 230 °C410 - 446 °F
Melt Temperature 220 - 240 °C428 - 464 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 80.0 - 85.0 °C176 - 185 °F
Dry Time 2 - 4 hour2 - 4 hour
Injection Pressure 68.6 - 108 MPa9950 - 15600 psi
Back Pressure 0.689 - 1.38 MPa100 - 200 psi
Screw Speed 60 - 80 rpm60 - 80 rpm
 
Descriptive Properties
UV Resistance<1 Delta E300 Hr. Ivory Color; ASTM D4459

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Starex® MP-0160R Metal Plating Grade ABS
LG Chemical Lupox® TE5000SP PBT+PC
LyondellBasell Hifax TYC 2128X 3001 Polypropylene Copolymer, Talc Filled
Lotte Advanced Materials Starex® MP-0670 ABS, Metal Plating Grade
Lotte Advanced Materials Infino® WP-1041 PC/ABS, Unreinforced Metal Plating Grade

PLBST001a / 195024

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.