MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Westlake 2070 Low molecular weight, film and medical grade, PVC suspension resin.
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Sheet Grade; PVC, Transparent

Material Notes: Westlake 2070 is a low molecular weight, film and medical grade, vinyl suspension resin. Designed for clear and opaque applications. This resin has good clarity, color and thermal stability. Kosher approved. Applications: Well suited for extruded sheet, bottles, fittings and other injection and blow molding products.

Information provided by Westlake Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.530 g/cc0.0191 lb/in³ASTM D1895
Volatiles <= 0.35 %<= 0.35 %
Particle Mesh Size 40 Mesh40 Mesh> 99.9% Through; ASTM D1921
 200 Mesh200 Mesh< 7% Through; ASTM D1921
Viscosity Measurement 0.690.69Inherent; ASTM D5225
 
Descriptive Properties
AppearanceFree Flowing White Powder
Cell ClassificationGP1-16360ASTM D1755
K-Value57ISO1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWESF8751 / 287861

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.