MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

W-50Mo Tungsten Alloy
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Refractory Metal; Tungsten Alloy

Vendors: Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 138 MPa
@Temperature 1650 °C
20000 psi
@Temperature 3000 °F
Stress-Relief Annealed
Elongation at Break 7.0 %7.0 %
Rupture Strength 83.0 MPa
@Temperature 1650 °C,
Time 36000 sec
12000 psi
@Temperature 3000 °F,
Time 10.0 hour
Stress-Relief Annealed
 
Component Elements PropertiesMetricEnglishComments
Molybdenum, Mo 50 %50 %
Tungsten, W 50 %50 %As balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carlson GOC 276 Nickel-Molybdenum-Chromium
Molybdenum TZC (Mo-1Ti-0.3Zr)
Molybdenum Mo-0.5Ti; M0-0.5Ti-0.02C (Molybdenum Alloy 362)
Overview of materials for Molybdenum Alloy
CuMoCu 13/74/13

MW909e / 193456

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.