MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMID® L-CF15 BK E70461 Nylon 12, Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Carbon Fiber Filler

Material Notes: VESTAMID® L-CF15 BK E70461 is a semi-crystalline UV-stabilised compound based on PA12 from which quick-connectors are produced by injection molding. The Polyamid compound ist especially suitable for Automotive and Mobility. Further advantages of VESTAMID® L-CF15 BK E70461are the characteristic properties of PA12, e.g., low water absorption, good dimensional stability and nearly constant mechanical properties at changing ambient humidity. Because of its semi-crystalline morphology VESTAMID® L-CF15 BK E70461 provides an excellent chemical resistance. VESTAMID® L-CF15 BK E70461 is supplied as cylindrical granules, ready for processing, in moisture-proof bags. Pigmentation may affect values. Preliminary data sheet.
Dry properties listed below
Industrial Sector: Automotive and Mobility
Processing: Injection molding
Delivery form: Pellets, Granules
Optics: Laser absorbing
Resistance to: Heat (thermal stability), UV / light / weathering
Electrical: Conductive
Conformity: Automotive
Additives: Carbon fibers
Applications: Quick-connectors
Processing: Casting
Special Characteristics: Halogen-free, Semi-crystalline, Light-stabilized, Medium viscosity
Color: Black
Additives: Conductive agent, Processing aids
Delivery form: Cylindrical pellets
Chemical Resistance: General chemical resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Water Absorption 1.27 %1.27 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 79.079.0ASTM D2240
Tensile Strength at Break 130 MPa18900 psiISO 527
Tensile Strength 130 MPa18900 psiISO 527
Tensile Strength, Yield 130 MPa18900 psiISO 527
Elongation at Break 3.70 %3.70 %Nominal; ISO 527
Elongation at Yield 3.50 %3.50 %ISO 527
Tensile Modulus 8.77 GPa1270 ksiISO 527
Charpy Impact Unnotched  5.10 J/cm²
@Temperature -40.0 °C
24.3 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
 5.30 J/cm²
@Temperature -30.0 °C
25.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.700 J/cm²
@Temperature -40.0 °C
3.33 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1840 ohm-cm1840 ohm-cmIEC 62631-3-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 °C352 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 179 °C354 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 169 °C336 °FISO 75-1/-2
Vicat Softening Point  176 °C
@Load 1.02 kg
349 °F
@Load 2.25 lb
50 K/h; ISO 306
 192 °C
@Load 5.10 kg
378 °F
@Load 11.2 lb
50 K/h; ISO 306
Glass Transition Temp, Tg 38.0 °C100 °FISO 11357-1/-2
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.0150 %0.0150 %ISO 15512
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7910 / 325042

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.