MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE

Material Notes: Description

Polytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties.
Application

TPP 615 is designed for applications such as body side claddings, rocker panels and grilles.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inas molded
 0.0080 cm/cm0.0080 in/in± 0.1 after 60 min. at 120°C
Melt Index of Compound 8.0 g/10 min8.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
Tensile Strength, Yield 13.8 MPa2000 psiASTM D638
Elongation at Yield 50 %50 %ASTM D638
Flexural Modulus 1.03 GPa150 ksiASTM D790
Gardner Impact 22.6 J
@Temperature -30.0 °C
16.7 ft-lb
@Temperature -22.0 °F
Impact 400400J/m, Charpy Notched Impact; ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 27.0 µm/m-°C
@Temperature -30.0 - 100 °C
15.0 µin/in-°F
@Temperature -22.0 - 212 °F
ASTM D696
 
Descriptive Properties
Heat Sag 1.78 mm1 hr at 120°C, 4 in over hang

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYTROPE™ TPP 608 Olefinic Elastomer
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer
Avient Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE))
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer
Dow INFUSE™ 9530 Olefin Block Copolymer

PASHU298 / 25262

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.