MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Meehanite AQ Flake Graphite Cast Iron
Categories: Metal; Ferrous Metal; Cast Iron; Gray Cast Iron

Material Notes: Type AQ is a wear and abrasion resisting iron that is readily machinable as-cast but may be "air-hardened" after machining with minimum risk of cracking or distortion. Type AQ is easily heat treated and locally hardened. Recommended for dies, punches, spinning mandrels and other hard wearing applications.

General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.

Information provided by Meehanite Marketing Association.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.34 g/cc7.34 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 280 - 550280 - 550Nominal
Tensile Strength, Ultimate 345 - 448 MPa50000 - 65000 psi
Tensile Strength, Yield 172 MPa25000 psi.01% permanent set
Modulus of Elasticity 152 GPa22000 ksi
Modulus of Rupture 0.641 GPa93.0 ksi
Compressive Strength 1380 MPa200000 psi
Poissons Ratio 0.330.33
Fatigue Strength 207 MPa30000 psi
Machinability 52 %52 %Dalcher
Shear Modulus 65.5 GPa9500 ksi
Izod Impact Unnotched 40.7 - 54.2 J
@Diameter 20.3 mm
30.0 - 40.0 ft-lb
@Diameter 0.798 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.1 µm/m-°C
@Temperature 37.8 - 538 °C
6.75 µin/in-°F
@Temperature 100 - 1000 °F
Shrinkage 1.3 - 1.5 %1.3 - 1.5 %Patternmaker Shrinkage

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gray Cast Iron, ASTM A 48 Class 40
ASTM class 20 Standard gray iron test bars, as cast
Overview of materials for Gray Cast Iron
Meehanite GM-60 Flake Graphite Cast Iron
United Cast Bar Unibar 200 Continuously Cast Iron

NMEE00 / 18221

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.