MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Dow Primacor® 5986 Ethylene acrylic acid copolymer
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Ethylene Acrylic Acid

Material Notes:
  • Low heat seal temperature
  • High gloss, excellent clarity
  • Excellent grease and oil resistance and excellent product resistance for flexible packaging applications
  • Complies with U.S. FDA 21 CFR 177.1310 (c)
PRIMACOR™ 5986 has excellent adhesion to metallic, cellulosic, glass and other polar substrates. It can be used effectively as a foil primer or laminating adhesive for polyethylene and metallized substrates.

Information provided by Dow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.958 g/cc0.0346 lb/in³ASTM D792
Melt Flow 13.8 g/10 min
@Load 2.16 kg,
Temperature 125 °C
13.8 g/10 min
@Load 4.76 lb,
Temperature 257 °F
ASTM D1238
Melt Index of Compound 300 g/10 min
@Load 2.16 kg,
Temperature 125 °C
300 g/10 min
@Load 4.76 lb,
Temperature 257 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050Compression molded; ASTM D2240
Tensile Strength at Break 9.65 MPa1400 psiCompression molded; ASTM D638
Elongation at Break 390 %390 %Compression molded; ASTM D638
Tensile Modulus 0.0331 GPa4.80 ksi2% Secant; Compression molded; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 77.2 °C171 °FDow Method (DSC)
Vicat Softening Point 42.2 °C108 °FASTM D1525
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Comonomer content, %20.5measured by direct titration

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Primacor® 5980I Ethylene Acrylic Acid (EAA)
Dow Primacor® 5990I Ethylene Acrylic Acid (EAA)
Dow Primacor® 3330 Ethylene Acrylic Acid (EAA)
Dow Primacor® 1321 Ethylene Acrylic Acid (EAA)
Dow Primacor® 3460 Ethylene Acrylic Acid (EAA)

PDOW1403 / 30621

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.