MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Piezo Kinetics 906 Lead Nickel Niobate Piezoelectric  (discontinued **)
Categories: Ceramic; Oxide; Piezoelectric

Material Notes: PKI 906 is slightly different in composition than the "general" PZT formulations. Its PZT-doped Lead Nickel Niobate composition was developed to enhance the d33 and dielectric properties of Navy Type VI materials. These enhanced properties make it the optimum choice for ultrasound or actuator applications. The increased dielectric constant allows engineers to use the material in smaller (higher frequency) applications while still maintaining the desired or necessary capacitance. The increased d33 allows for higher displacement applications.

Elastic Compliance s11E (x 10-12 m²/n): 15.4.
Elastic Compliance s33E (x 10-12 m²/n): 18.2.

Property data at 25°C. Information supplied by Piezo Kinetics, Inc.

Key Words: PKI 906, Lead Nickel Niobium Oxides
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 55.0 GPa7980 ksi
Poissons Ratio 0.220.22
Shear Modulus 23.0 GPa3340 ksicalculated
 
Electrical PropertiesMetricEnglishComments
Curie Temperature 150 °C302 °F
Dielectric Constant 5500
@Frequency 1000 Hz
5500
@Frequency 1000 Hz
Dissipation Factor 0.023
@Frequency 1000 Hz
0.023
@Frequency 1000 Hz
Piezoelectric Longitudinal Coupling Factor, k33 0.700.70
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -310-310
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 700700
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 13.613.6
Piezoelectric Planar Coupling Factor, kp 0.600.60
Piezoelectric Mechanical Q 5555
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 660660
Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N -6.40-6.40
Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N 14.414.4
Piezoelectric Transverse Coupling Factor, k31 0.350.35
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Piezo Kinetics 700 Lead Zirconate Titanate Piezoelectric
Piezo Kinetics PKI 804 Navy Type III Lead Zirconate Titanate Piezoelectric
Channel Industries 5400 Lead Zirconate Titanate Piezoelectric
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
Carpenter Super Invar 32-5

CPKI50 / 1715

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.