MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Stat-Rite® S-680 Static Control PETG Alloy
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: Stat-Rite® S-680 is a static dissipative PETG alloy. Stat-Rite® M-680 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation even when extruded, injection molded or thermoformed into components.

Features:

  • Permanent static dissipative performance
  • Humidity insensitive
  • Ultra-clean: low off-gassing, low ionic contamination
  • Colorable
  • Durable: Can be used repeatedly.

Applications:

  • Hard disk packaging
  • Medical device packaging
  • Electronic component handling

Available in Americas, Europe, Middle East, Africa, India and Asia

Data provided by Lubrizol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 28.3 MPa4100 psiASTM D638
Elongation at Break 350 %350 %ASTM D638
Tensile Modulus 1.10 GPa160 ksiASTM D638
Flexural Modulus 1.24 GPa180 ksiASTM D790-92
Izod Impact, Notched 9.61 J/cm18.0 ft-lb/inASTM D256-92
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+9 ohm-cm2.00e+9 ohm-cm50% RH; ASTM D257
Surface Resistance 8.00e+8 ohm8.00e+8 ohmESD S11.11; 12 % R.H.
Surface Resistivity per Square 2.00e+9 ohm2.00e+9 ohmASTM D257
Static Decay 0.010 sec0.010 secFTMS-101C; 12% R.H., (+5000 V to 50 V)
 0.010 sec0.010 secFTMS-101C; 12% R.H., (-5000 V to -50 V)
 0.10 sec0.10 secCharged Plate Monitor; 50% R.H. MD, (+1000 V to 10 V)
Tribocharge 10 V10 VNitrile Glove - BFG Test Method
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C140 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FASTM D648
 
Descriptive Properties
ColorLight Blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Stat-Rite® M-690 Static Control PETG Alloy
Eastman Eastar K3000 PETG Copolyester
Mitsubishi Chemical Advanced Materials Ertalyte™ PET Polyester-semi-crystalline thermoplastic, extruded
Overview of materials for PETG Copolyester
Plaskolite Mustang PETG Sheet

PNOVEON24 / 55455

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.