MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, at 50% RH  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 20% Glass Fiber Reinforced

Material Notes: AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent creep resistance and low moisture absorption are also characteristic of this resin. AMODEL A-1115 HS resin can be easily processed using conventional equipment and methods.

This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.

MatWeb has an entry for this material dry as molded.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³dry as molded
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 112 MPa16200 psiASTM D638
Elongation at Break 1.9 %1.9 %ASTM D638
Tensile Modulus 8.30 GPa1200 ksiASTM D638
Flexural Yield Strength 161 MPa23400 psiASTM D790
Flexural Modulus 6.20 GPa899 ksiASTM D790
Compressive Yield Strength 190 MPa27600 psiASTM D695
Shear Strength 81.0 MPa11700 psiASTM D732
Izod Impact, Notched 0.360 J/cm0.674 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cmASTM D257
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
ASTM D150
 4.4
@Frequency 60 Hz
4.4
@Frequency 60 Hz
ASTM D150
Dielectric Strength 19.0 kV/mm483 kV/inASTM D149
Dissipation Factor  0.0080
@Frequency 60 Hz
0.0080
@Frequency 60 Hz
ASTM D150
 0.023
@Frequency 1e+6 Hz
0.023
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 115 sec115 secASTM D495
Comparative Tracking Index 550 V550 V
 
Processing PropertiesMetricEnglishComments
Melt Temperature 321 - 343 °C610 - 649 °FInjection

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOLVT22 / 21318

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.