MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Beijing Evergrow Resources PTFE Skived Sheet Tape
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: PTFE resin is first molded into work-blank and then skived. The PTFE resin skived sheet & tape are highly dielectric. Chemical resistant and not aging. They have a wide range of operation temperature.

Applications:
Lining, sealing and oil-less lubricating material and dielectric at any frequencies. Capacitor dielectric, wire isolation, electrical instrument isolation.

Information provided by Beijing Evergrow Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.10 - 2.30 g/cc0.0759 - 0.0831 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break >= 150 %>= 150 %
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 10.0 kV/mm>= 254 kV/in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Fluorosint™ 500 PTFE, synthetic mica-filled PTFE, compression molded
Mitsubishi Chemical Advanced Materials Fluorosint™ MT-01 PTFE reinforced with carbon fibers and organometallic fillers
Beijing Evergrow Resources PTFE Sheet
Mitsubishi Chemical Advanced Materials Fluorosint™ 207 PTFE, Compression Molded Synthetic Mica-filled PTFE
RTP Company RTP 1001 GB 15 TFE 5 Polybutylene Terephthalate (PBT), Glass Fiber - Glass Bead - PTFE Lubricated

PBEIJ030 / 90099

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.