MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Danquinsa DANPOL® PES-980 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: DANPOL PES-980 is a copolyester adhesive with high crystallization properties in form of granules. This copolyester is an optimal adhesive raw material for the application as hot-melt or solved in organic solvents. The granules of DANPOL PES-980 can be grinded to powder for powder hot-melt coatings.

Application: DANPOL PES-980 will be used for air, oil and fuel automotive filters. It offers a better adhesion on aluminum and conventional plastic materials. DANPOL PES-980 does not contain any toxic ingredients.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³DIN 53.479
Brookfield Viscosity 30000 - 40000 cP
@Temperature 232 °C
30000 - 40000 cP
@Temperature 450 °F
Thermosel, Melting
Melt Flow 200 g/10 min
@Temperature 180 °C
200 g/10 min
@Temperature 356 °F
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 3.0<= 3.0[mg KOH/g]
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 14.0 - 15.0 MPa2030 - 2180 psi
Elongation at Break 90 %90 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 170 - 174 °C338 - 345 °FKofler, Ring & Ball
Softening Point 161 - 166 °C322 - 331 °FDSC
Ring & Ball Softening Point 170 - 174 °C338 - 345 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 220 - 240 °C428 - 464 °FWorking temp
Cure Time 0.0333 min0.000556 hourRecrystallisation
 0.133 - 0.183 min0.00222 - 0.00306 hourOpen time
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AspectGranules
Hydroxyl value3-5 mg KOH/g
TypeCopolyester

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ167 / 294587

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.